E44-335 · Excessive Piping Resistance and Pressure Drop · Slurry pipe at 15% solids · ★★
Particulate wear shrinks the bore 2mm/yr; after 3 years v rises 12%, hf rises 25%, and the end pressure drops
[Mechanism] Erosion by 15% solids shrinks d by 2mm/yr and raises v.
[Calculation] hf∝v² rises 25%, dropping the end pressure.
[Design Omission] No wear-resistant pipe and no upsizing for wear allowance - erosion kept resistance high.
1) Use wear-resistant pipe (ceramic/alloy lining) to hold annual shrinkage ≤0.5mm, since 15% solids shrank 2mm/yr, raised v 12% and hf 25%, resisting wear;
2) Oversize the design bore to leave a wear allowance, since the bore shrinks in service, leaving margin;
3) Hold solids concentration ≤10%, since high concentration wears badly, controlling concentration;
4) Add a cyclone to pre-remove coarse particles, since coarse grains wear severely, removing coarse grit;
5) Periodically measure the bore to catch shrinkage early, since it creeps unnoticed, measuring the diameter;
6) Compute in-service hf with the shrunk bore, since a nominal bore understates the drop, computing for real;
7) Boost pump head to cover the added resistance, since the end needs pressure, adding head;
8) Include wear in the design, since the missing control was the root cause of shrinkage, closing the loop at design.
GB/T 20801.3-2020 Design code for industrial metallic piping