E44-268 · Valve Selection and Internal Leakage · Needle valve J13W-160P DN10 · ★★
Downstream of the throttle orifice, cavitation pits reached 0.3mm deep and flow drifted by 10%; the valve needle eroded out of round.
[Cavitation] Throttling drops the local pressure until p < the saturated vapor pressure; bubbles collapse and erode the valve needle.
[Vena Contracta] At the throat the velocity v=√(2Δp/ρ) exceeds 30m/s, causing severe erosion.
[Design Omission] No control of the throttling pressure-drop ratio and no erosion-resistant material — the needle valve eroded.
1) Limit the single-stage pressure drop to Δp/p1≤0.3 to avoid cavitation; beyond this p falls < the vapor pressure and collapsing bubbles pit the needle 0.3mm deep, so control the drop;
2) Change the needle to cemented carbide or ceramic; the original material eroded out of round under the high-velocity flow and drifted flow by 10%, so make it erosion-resistant;
3) Use multi-stage throttling to split the pressure drop; a single large drop erodes easily, so step the drop down gradually;
4) Add a downstream diffuser to stabilize the flow; v>30m/s at the vena contracta erodes, so diffuse and slow it;
5) Periodically measure flow drift to detect erosion; erosion causes drift, so diagnose early;
6) For high pressure differentials switch to a cage-guided valve; the cage splits the pressure drop more evenly, stabilizing the flow;
7) If the medium carries gas, vent it before throttling; gas promotes cavitation, so clean the flow first;
8) Include the pressure-drop ratio in selection; the lack of control was the cause of erosion, so gate it at design.
GB/T 12224-2015 Steel valves — General requirements