E44-285 · Valve Selection and Internal Leakage · Soft-seated gate valve Z45X-10 DN100 · ★★
The wedge rubber aged and crazed; it would not seal and leaked 1L/min, cracking after 3 years of service.
[Aging] Under warm water and ozone the rubber lost elasticity and crazed.
[Crack] Cracks break the sealing band and leak.
[Design Omission] No aging-resistant rubber was chosen and the service temperature and humidity were not controlled — the soft-seated gate valve cracked.
1) Choose an aging-resistant rubber such as EPDM; the original rubber crazed in 3 years and would not seal with 1L/min leakage, so make it weather-resistant;
2) Keep the medium temperature within the rubber rating (e.g. ≤80℃); high temperature accelerates aging, so control the temperature;
3) Avoid ozone environments or add a cover; ozone promotes cracking, so isolate it;
4) Replace the wedge periodically (by years); aging has a finite life, so replace on schedule;
5) Run tightness tests to find cracking leaks; cracks grow, so verify the seal;
6) Switch to a metal hard seat to avoid aging; hard faces do not age, so make it durable;
7) Vent the valve pit to lower humidity; heat and moisture promote aging, so ventilate;
8) Bring rubber grade and life into selection; the mismatch was the cause of cracking, so gate it at design.