E44-290 · Valve Selection and Internal Leakage · Vacuum diaphragm valve GM-1 DN25 · ★★
The vacuum chamber leak rate was 1×10⁻³Pa·m³/s (requirement ≤1×10⁻⁵); the vacuum could not be pulled and the product oxidized.
[Leak] Micro-roughness on the sealing face and rubber permeation let atmosphere in.
[Permeation] Rubber gas permeability causes a slow leak.
[Design Omission] No metal seal and no leak-rate control — the vacuum valve leaked.
1) On high-vacuum sections switch to a metal seal (copper gasket / knife edge); the gas-permeable rubber gave a 1e-3 leak rate over the 1e-5 requirement and would not pull vacuum, so seal with metal;
2) Choose a low-permeability rubber (fluorocarbon) to cut permeation; rubber permeation is the slow-leak source, so use low-permeation material;
3) Select by leak rate and run a helium mass-spectrometer leak test; leak rate is hard to notice, so leak-test;
4) Keep the sealing face Ra≤0.8 for full contact; roughness leaks, so make it smooth;
5) Periodically retighten the flanges to hold seal; loosening leaks, so retighten;
6) Add a fore-vacuum valve for staged pumping; a single valve cannot reach high vacuum, so stage it;
7) Control ambient humidity to cut oxidation; in-leak brings oxygen, so control the environment;
8) Bring leak rate into the vacuum design; the lack of control was the cause of leakage, so gate it at design.
JB/T 10762-2007 Vacuum valves