Weld Spatter Trapped in the Sealing Face Causes Leakage

E44-1036 · Valve Selection & Internal Leakage · Sealing Face · ★★

Problem Symptom

Trapped spatter, leakage, dripping

Root Cause

[Mechanism] Weld spatter and dirt were trapped in the sealing face during installation, forming a linear channel after closure through which the medium seeped.
[Calculation] DN100 flanged valve with two spatter inclusions of 0.3mm each in the sealing face; after closure the linear leak was 80mL/min and the local sealing specific pressure was only 0.4MPa against the 1.0 required.
[Design Omission] The sealing faces were not cleaned, no closure check was made, and the medium was not filtered.

Correct Solution

1) Disassemble the valve and clean the sealing faces (remove the spatter and polish to Ra<=1.6); the spatter caused the linear leak and cleaning the face makes it flat, stopping the leak;
2) Verify the flatness of the sealing face (<=0.05mm over the full circumference); a damaged face leaks and verifying the flatness makes it close, sealing the joint;
3) Change to a better gasket (spiral-wound metal replacing asbestos); the old gasket compressed unevenly and leaked and the new gasket distributes the load evenly, sealing the joint;
4) Tighten the bolts uniformly (three diagonal passes, torque spread <=10%); an uneven load leaks and uniform tightening makes it flat, equalising the pressure;
5) Carry out a tightness test (0.6MPa, soap solution, no bubbles); micro-leakage is hard to see and a tightness test reveals it, detecting the micro-leakage;
6) Fit a medium filter upstream (100 micron); heavy spatter damages the face and filtering keeps it clean, protecting the face;
7) Keep the medium clean in operation (free of weld spatter); spatter causes leakage and keeping it clean protects the face, preventing leakage in operation;
8) Write the face cleaning and flatness verification into the assembly card; the root cause of the trapped spatter was an uncleaned face with no inspection, so the assembly card closes the loop.

Checklist

References

GB/T 12224-2015 Steel Valves - General Requirements