MOULDLKnowledge Base3D Model DownloadsMembership
中文版Model Store »
Knowledge Base › Fluid System Error Cases › Crushed Graphite Spiral-Wo
HomeModels
Table of contents

Knowledge Base Home

📐 Standard Data

🧮 Calculators

📖 Selection Guides

🏭 Material Grades

❓ Engineer FAQ

🗂 Quick-Reference Categories

❌ Error Case Studies

📚 Technical Articles

Crushed Graphite Spiral-Wound Gasket Causes Leakage

E44-565 · Seal Leakage · Flange Gasket · ★★

Problem Symptom

Leakage, gasket thickness reduced 40%, crushed

Root Cause

[Mechanism] Over-tightening crushes the gasket.
[Calculation] A pressure of 120MPa against the 90MPa allowable reduces the thickness by 40%, the rebound is lost and it leaks.
[Design Omission] The torque was not controlled, the pressure was not limited, and a thicker gasket was not selected - the gasket was crushed.

Correct Solution

1) Control the tightening torque at 70N-m (based on the allowable specific pressure of the gasket); the original 120N-m against 90N-m reduced the gasket thickness by 40%, lost the rebound and leaked, so limiting the pressure stops the crushing;
2) Limit the pressure to <=90MPa (back-calculated from the torque and the gasket factor); above that the gasket is crushed, so limiting the pressure prevents it;
3) Select a thicker gasket (3mm, low preload specific pressure); a thin gasket crushes easily, so thickening it adds capacity;
4) Fit a load-limiting washer (a torque-limiting nut); over-tightening crushes the gasket, so the limiting washer caps the force;
5) Tighten evenly with a torque wrench (error within +/-5%); an uneven load crushes the gasket locally, so even tightening prevents it;
6) Control the tightening rate and tighten progressively (in passes); tightening sharply applies an instantaneous crushing load, so slow progressive tightening avoids it;
7) Set a routine thickness inspection (caliper, replace when the reduction exceeds 20%); the thickness reduces gradually and then crushes, so the thickness is inspected;
8) Write the torque control and the pressure limit into the assembly card; the original absence of pressure control was the root cause of the crushing, so the assembly card closes the loop.

Checklist

References

HG/T 20610-2017 Spiral Wound Gaskets for Steel Pipe Flanges