E44-457 · Filter Clogging and Contamination · Bag Filter 25μm · ★★★
The filter-bag weld cracked; outlet solids concentration was 0.5%, >50× the inlet 0.01%; downstream product was contaminated and the batch had to be reworked.
[Mechanism] The bag weld cracks under pulsating pressure, creating a short-circuit bypass.
[Calculation] A 2mm crack gives a bypass rate = crack area / total filter area = 5%, and outlet concentration rises from 0.01% to 0.5%.
[Design Omission] No integrity leak test was done and the bag clamp was not tight; the crack went undetected and caused leakage.
1) Replace the bag and perform a bubble leak test to confirm no cracks, because the original weld had cracked, bypass was 5% and outlet was 0.5%, thereby leak-testing to prevent leakage;
2) Set the bag-clamp torque to the specified value against loosening, because a loose clamp opens the weld and cracks it, thereby tightening the clamp;
3) Install online turbidity meters on inlet and outlet, because concentration rises after a crack and is detectable, thereby monitoring concentration;
4) Add a coarse pre-filter ahead of the bag to reduce its load, because heavy loading causes cracking, thereby reducing load;
5) Change the bag material to pulse-resistant polyester, because the original material was not pulse-resistant, thereby making it pulse-resistant;
6) Compare particle counts before and after each batch, because without comparison leakage is hard to detect, thereby checking by comparison;
7) Limit inlet velocity to prevent bag erosion, because flow scouring causes cracking, thereby limiting velocity;
8) Write leak testing into the bag-replacement procedure, because the original lack of testing is the root cause of cracking, thereby enforcing procedural control.
GB/T 26114-2010 Filters for liquid filtration