E44-479 · Filter Clogging and Contamination · Mold-Temperature-Controller Filter 50μm · ★★
Hard water caused calcium scale on the screen, Δp=0.08MPa, uneven mold temperature, and product shrinkage
[Mechanism] CaCO₃ scale deposits occupy the pores.
[Calculation] Hardness of 300mg/L grows scale 0.5mm per month, shrinking pore size 40%, raising v, and reaching Δp=0.08.
[Design Omission] No water softening and no scale inhibitor, so calcium scaling plugged the screen.
1) Soften the make-up water to keep hardness <50; since 300 caused scaling, 40% pore shrinkage, and Δp=0.08, softening prevents scale;
2) Add a scale inhibitor to suppress crystallization; since crystals cause plugging, inhibition prevents it;
3) Acid-wash periodically to remove scale; since scale builds gradually, acid washing removes it;
4) Add a Δp alarm; since exceeding it causes uneven temperature, the alarm warns;
5) Make the screen removable for quick replacement; since plugging requires changes, quick swaps reduce downtime;
6) Control water temperature to prevent evaporative concentration; since concentration causes scaling, temperature control prevents it;
7) Flush the bypass on schedule; since deposits cause plugging, scheduled flushing removes them;
8) Write softening and scale inhibition into the mold-temperature procedure; since water was never softened, the root cause of scaling, the procedure provides the check.
GB/T 26114-2010 Filters for liquid filtration