E44-171 · Heat-Exchanger Fouling and Insufficient Heat Transfer · Shell-and-Tube Heat Exchanger · ★★
No chemical treatment was applied; calcium scale is 1.5mm thick, heat-transfer coefficient K drops 30%, and outlet temperature fails spec.
[Fouling] Calcium and magnesium deposit as scale, adding thermal resistance.
[K Drop] A 1.5mm scale layer cuts K by 30%.
[Design Omission] No water treatment was provided and no fouling margin was left, leading to insufficiency.
1) Apply chemical dosing / softening to cooling water to prevent scale, since a 1.5mm calcium layer cuts K by 30%, thus treating for scale inhibition;
2) Leave a fouling thermal-resistance margin in design, since scale inevitably forms, thus keeping K up with margin;
3) Provide online cleaning (sponge balls / brushes) to remove scale, since scale gradually thickens, thus cleaning on schedule;
4) Monitor inlet/outlet temperature difference to detect fouling, since a K drop changes ΔT, thus monitoring ΔT;
5) Periodically chemically clean to restore K, since hardened scale is hard to flush, thus cleaning on schedule;
6) Monitor and alarm on water hardness, since hard water scales faster, thus monitoring hardness;
7) Measure heat-transfer coefficient ≥ design on test run, since design requires verification, thus confirming delivery;
8) Bring water treatment into heat-exchanger design, since the original lack of treatment was the root cause of fouling, so design must include it.
GB/T 151-2014 Heat exchangers