E44-173 · Heat-Exchanger Fouling and Insufficient Heat Transfer · Reactor Heating Coil · ★★
Process fluid cokes on the tube wall 2mm thick, raising thermal resistance, slowing heating, and increasing time by 40%.
[Coking] High-temperature process fluid cokes on the tube wall.
[Resistance Rise] A 2mm coke layer makes thermal resistance large.
[Design Omission] No wall scraping / decoking was provided and wall temperature was not controlled, leading to insufficiency.
1) Fit mechanical wall scraping on the coil to prevent coke adhesion, since 2mm of coke raises resistance and slows heating, thus keeping the wall clean by scraping;
2) Keep wall temperature below the coking temperature, since high temperature cokes, thus controlling temperature;
3) Choose an easy-to-clean design for coke removal, since hardened coke is hard to clean, thus making it easy;
4) Periodically chemically decoke to restore heat transfer, since coke gradually thickens, thus cleaning on schedule;
5) Monitor the heating curve to detect coking, since slow heating is a precursor, thus watching the curve;
6) Pre-treat the process fluid to reduce coke precursors, since impurities cause coking, thus pretreating;
7) Measure heating to design on test run, since design requires verification, thus confirming delivery;
8) Bring coke prevention and decoking into heating design, since the original omission was the root cause of coking, so design must include it.
GB/T 151-2014 Heat exchangers