E44-516 · Heat Exchanger Fouling and Insufficient Heat Transfer · Reactor Coil Carbon Steel · ★★
Coil scaling, slow temperature control, unstable reaction
[Mechanism] Process-fluid scale deposits on the coil.
[Calculation] Rf=0.4 cuts K by 40%, slows temperature-control response, and causes a ±5℃ swing.
[Design Omission] No scale cleaning and no pretreatment, so scaling occurs.
1) Clean the coil on schedule to remove scale (CIP each batch / cycle); process scale on the coil (Rf=0.4, K drop 40%, slow control response, ±5℃ swing), so scheduled cleaning restores K and stabilizes control;
2) Pre-filter the process fluid to remove solids; suspended solids bond to the tube and aid scaling, so pre-filtration cuts deposition;
3) Monitor temperature-control response (heat-up / cool-down rate); scaling slows response as a symptom, so response monitoring warns of scale;
4) Fit a temperature-swing alarm (±3℃); scale causes unstable control and poor reaction, so the alarm prevents instability;
5) Change coil material to non-stick (polished / specialty alloy); scale bonds easily to carbon steel, so a non-stick surface reduces deposition and eases cleaning;
6) Raise process-fluid velocity to prevent settling; components settle in low-velocity zones, so higher velocity suppresses scaling;
7) Add a scale/dispersant inhibitor; crystal nuclei bond to the wall and form scale, so inhibitor reduces deposition;
8) Write cleaning and pre-filtration into the reactor procedure; the original design omitted cleaning and pre-filtration, the root cause of scale, so the procedure closes the loop.
GB/T 151-2014 Heat exchangers