E44-517 · Heat Exchanger Fouling and Insufficient Heat Transfer · Closed-Circuit Cooling Tower Coil · ★★
Coil scaling, outlet water-temperature rise, cooling-efficiency loss
[Mechanism] Circulating-water scale deposits on the coil.
[Calculation] Rf=0.3 lowers K, raises outlet by 5℃, and cuts cooling efficiency by 20%.
[Design Omission] No chemical dosing and no flushing, so scaling occurs.
1) Dose scale/corrosion inhibitor to keep Rf<0.1; circulating-water calcium scale bonds to the coil (Rf=0.3, outlet +5℃, cooling efficiency −20%), so dosing lowers Rf and restores K;
2) Schedule coil back-flushing (periodic reverse wash); scale builds and hardens over time, so back-flushing removes it;
3) Fit an outlet-temperature alarm (on +3℃ over limit); scaling causes insufficient cooling and temperature rise, so the alarm prevents efficiency loss;
4) Stabilize water quality (control pH / alkalinity); unstable water scales readily, so stabilization suppresses it;
5) Raise flow velocity to prevent settling (≥1.2 m/s); suspended calcium settles in low-velocity zones, so higher velocity suppresses scaling;
6) Use a side-stream filter to cut suspended solids; settled solids aid scaling, so side filtration reduces the load;
7) Inspect scale thickness on schedule (thickness gauge / visual); scale thickens and lowers K, so inspection guides cleaning;
8) Write dosing and back-flushing into the cooling-tower procedure; the original design omitted dosing and back-flushing, the root cause of scale, so the procedure closes the loop.
GB/T 151-2014 Heat exchangers