E44-524 · Heat Exchanger Fouling and Insufficient Heat Transfer · Condensate Exchanger Carbon Steel · ★★
Oxygen-corrosion pitting, plugging, leakage, heat-transfer loss
[Mechanism] Oxygen in condensate causes pitting.
[Calculation] Oxygen content >0.1 mg/L causes pitting, 30% plugging, leakage and K drop.
[Design Omission] No deaeration and no corrosion inhibition, so oxygen corrosion occurs.
1) Deaerate and inhibit condensate to keep oxygen <0.05 mg/L; oxygen >0.1 mg/L pits carbon steel (30% plugging, leakage, K drop), so deaeration and inhibition prevent pitting and restore flow;
2) Change material to stainless steel (316L); carbon steel resists oxygen corrosion poorly and perforates, so the change extends life;
3) Fit leakage monitoring (flow difference); corrosion breakthrough leaks and loses water, so leak monitoring gives early detection;
4) Control pH to prevent corrosion (9–10); acidity raises corrosion rate, so pH control suppresses corrosion;
5) Inspect pits on schedule (thickness gauge / pressure test); corrosion enlarges pits and leaks, so inspection guides plugging;
6) Control velocity to prevent erosion-corrosion (≤2 m/s); high velocity promotes erosion pitting, so velocity control reduces corrosion;
7) Provide a bypass for continued operation (during maintenance); internal leakage forces shutdown and disrupts the system, so a bypass keeps it running;
8) Write deaeration and inhibition into the condensate procedure; the original design omitted deaeration, the root cause of corrosion, so the procedure closes the loop.