E44-550 · Heat Exchanger Fouling and Insufficient Heat Transfer · Sulfur Recovery Heat Exchanger - Carbon Steel · ★★
Sulfur condenses and deposits, blockage, flow drop, uneven temperature
[Mechanism] Sulfur condenses and deposits on the walls.
[Calculation] Excessively low wall temperature causes sulfur to condense and deposit, 30% blockage, and uneven temperature.
[Design Omission] No wall-temperature control and no flushing were provided, causing blockage.
1) Control wall temperature (≥ sulfur dew point +15℃) to prevent sulfur condensation; because excessively low wall temperature causes sulfur to condense and deposit, 30% blockage, and uneven temperature, temperature control prevents condensation and restores the flow passage;
2) Schedule steam blowing (blow down every 8 h, force-blow when Δp>0.1 MPa); because sulfur buildup narrows channels and pressure rise precedes complete blockage, periodic blowing restores the flow area;
3) Add flow monitoring (alarm when flow <85% of design); because sulfur condensation blockage first shows up as a flow drop before flow stops, monitoring flow gives early warning;
4) Add heat tracing and insulation (shell-and-tube heat tracing / insulation layer); because cold conditions cause sulfur condensation and heat tracing raises wall temperature to prevent it, insulation prevents freeze-condensation;
5) Raise flow velocity (≥1.2 m/s) to prevent stagnation; because sulfur vapor condenses and deposits in low-velocity zones and hardens over time, higher velocity reduces residence time and suppresses condensation;
6) Use sulfur-resistant materials (316L / nickel-based alloy); because sulfur corrodes ordinary materials and corrosion pits promote deposition, sulfur-resistant material extends life and suppresses deposition;
7) Schedule thickness inspection (measure wall thickness / visual every two months); because sulfur gradually thickens and worsens blockage and uneven temperature, quantitative measurement guides blowing;
8) Write wall-temperature control and steam blowing into the sulfur recovery procedure; because the original design omitted temperature control and blowing, the root cause of condensation, the procedure enforces control.
GB/T 151-2014 Heat exchangers