E44-709 · Hydraulic System Contamination and Crawling · Hydraulic Hose · ★★★
Aging and bursting, oil spray
[Mechanism] The aged hose bursts.
[Calculation] Aging causes bursting.
[Design Omission] No replacement, no protection, and no inspection - a design defect leading to aging.
1) Replace hoses on a life limit (3 years / 8000h); the original aged hose burst, with the pressure collapsing to 60% of rated and oil spraying out, so life-limited replacement prevents bursting;
2) Shield from sunlight to prevent aging (protective cover, avoid UV); sunlight ages the hose, so shielding slows aging and extends life;
3) Control temperature to prevent aging (≤80℃); heat ages the hose, so temperature control slows aging and extends life;
4) Select aging-resistant hoses (synthetic rubber, weather-resistant); degraded hoses burst, so weather-resistant material extends life and prevents bursting;
5) Inspect for cracks (visual + pressure test; replace at any crack); gradual aging is invisible, so inspection catches it early for early warning;
6) Limit pressure against overpressure (≤90% of rated); overpressure bursts the hose, so limiting keeps it safe and the pressure stable;
7) Protect the hose against abrasion (sleeves, avoid rubbing); abrasion accelerates aging, so protection extends life;
8) Write life-limited replacement and sun shielding into the maintenance card (replacement record); since lack of replacement was the root cause of aging, closing the loop in the maintenance card gives maintenance control.
GB/T 3766-2015 General technical conditions for hydraulic systems