E44-710 · Hydraulic System Contamination and Crawling · Bent Pipe · ★★
Bend cracking, leakage
[Mechanism] Bend stress causes cracking.
[Calculation] Stress causes cracking.
[Design Omission] No gentle bend, no support, and no inspection - a design defect leading to stress.
1) Increase the bend radius for a gentle bend (R≥3D, no wrinkling); the original tight bend concentrated stress and cracked and leaked, so a gentle bend lowers the stress;
2) Add supports and hangers against vibration (spacing ≤1.5m, fixed); vibration causes cracking, so supports damp the vibration;
3) Check bend wall thickness against thinning (wall thickness ≥90% of design, measured); thinning causes cracking, so checking ensures adequate strength;
4) Select tough material tubing (normalized 20 steel, Akv≥40); brittle material cracks, so tough material resists and extends life;
5) Inspect for cracks (penetrant testing; replace at any crack); gradual cracking is invisible, so inspection catches it early for early warning;
6) Control pressure against overpressure (≤90% of rated); overpressure cracks the pipe, so limiting keeps it safe and pressure stable;
7) Accommodate thermal expansion to prevent cracking (expansion compensator, allow movement); expansion cracks the pipe, so compensation relieves it and preserves the shape;
8) Write gentle bends and supports into the assembly card (bend record); since lack of a gentle bend was the root cause of stress, fixing it in assembly gives assembly oversight.
GB/T 3766-2015 General technical conditions for hydraulic systems