E44-085 · Piping Supports and Thermal Expansion · Hot oil pipeline · ★★
The seized sliding support prevents thermal expansion from releasing; the pipe bending stress is 1.5× the allowable and it deforms
[Seizing] The support rusts and seizes, raising friction so the pipe cannot slide to release its thermal elongation.
[Calculation] The 0.12m thermal elongation is restrained, making the bending stress 1.5× the allowable.
[Design Omission] No rust protection was applied to the support and no sliding clearance was left — so the stress exceeded the allowable.
1) Provide the support with a rust-proof sliding surface (a stainless-steel plate or coating): because rust seizure raises friction and stops the pipe sliding, rust protection keeps it sliding so the thermal elongation releases freely;
2) Leave thermal sliding allowance (a gap on the support bearing face): because the allowance lets the pipe elongate freely without seizing, the stress does not accumulate;
3) Set guides (restrain laterally, release axially): because the guides control the direction while axial movement stays free, the thermal elongation is released and whipping is prevented;
4) Reduce the restraint stiffness (a low-friction sliding surface): because a low friction coefficient lowers the release resistance and the stress, the pipe bending stress returns to the allowable;
5) Verify the bending stress (σ≤ the allowable): because the 1.5× overstress needs quantifying and the check verifies it, safety is confirmed;
6) Monitor at hot state (check for free elongation on heat-up): because seizure is progressive and monitoring gives early warning, rust protection is timely;
7) Verify free expansion at trial run (no abnormal bending): because the stress bending is the result and must be measured, acceptance follows;
8) Include the sliding allowance in the support design: the original lack of sliding allowance caused the seizure and overstress, so sliding is provided at the design stage.
GB/T 20801-2020 Pressure piping code