Knowledge Base › Fluid Systems Error Case › Throttling Orifice Cavitation Noise

Throttling Orifice Cavitation Noise

E44-843 · Throttling Noise and Vibration · Throttling orifice · ★★★

Problem Description

A DN150 throttling orifice with 0.9MPa upstream and 0.18MPa downstream had a cavitation number σ=0.27, 90dB(A) noise, and pitting

Root Cause

[Mechanism] At the orifice's vena contracta the pressure drops below the vapor pressure and bubbles form; they collapse in the downstream high-pressure zone, striking the metal to radiate noise and pit it.
[Calculation] σ=(p2-pv)/(p1-p2)=(0.18-0.02)/(0.9-0.18)=0.22<1.0 enters severe cavitation; the collapse impact >1000MPa.
[Design Omission] No backpressure raise, no cavitation-number check, no cavitation-resistant material selected.

Corrective Solution

1) Raise the backpressure (add a restrictor after the orifice to raise p2 from 0.18 to 0.55MPa and σ→1.2), since the original σ0.22 cavitated and pitted and raising the pressure prevents erosion;
2) Verify the cavitation number (σ≥1.3 margin), since low pressure erodes and verification avoids it, thus verifying σ;
3) Replace with a cavitation-resistant trim (carbide with a Stellite hardfacing layer), since the original carbon steel was eroded through by the collapse impact and the replacement resists it, thus replacing the part;
4) Add flow guiding and stabilization (10D straight pipe upstream + guide vanes), since disturbed flow creates local low pressure that erodes and guiding steadies it, thus guiding the flow;
5) Inspect the erosion (borescope the pits downstream of the orifice, alarm at pit depth >0.5mm), since gradual erosion thins the wall and early detection catches it, thus inspecting erosion;
6) Run a cavitation test (step down the pressure and measure noise and erosion rate), since the lack of testing left the erosion undetected and the test reveals the threshold, thus cavitation testing;
7) Control and split the pressure drop (multi-stage orifices, single stage Δp≤0.3MPa), since concentration erodes and splitting eases it, thus controlling the drop;
8) Write back-pressure increase and σ verification into the calculation sheet, since the original lack of increase is the root cause of pitting and locking it in closes the loop, thus controlling it in the calculation.

Checklist

Reference

GB/T 17213.1-2015 Industrial-process control valves

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL