E45-347 · Environmental Protection and Temperature/Humidity · Strain Sensor · ★★
An intertidal-zone sensor goes through alternating wet and dry cycles; salt repeatedly concentrates and crystallizes, accelerating corrosion of the housing and leads
[Mechanism] Alternating wet and dry cycles evaporate and concentrate the residual salt water; the crystals expand and damage the coating, and when wet the high-concentration brine accelerates electrochemical corrosion.
[Calculation] Wet-dry cycling can raise the local salt concentration to saturation (about 26%), and the corrosion rate becomes 2~3 times that of continuous immersion.
[Design Omission] The alternating wet-dry duty was not evaluated, and the protection does not withstand salt crystallization.
① Salt-resistant coating: apply a thick-film epoxy plus polyurethane topcoat to the housing → resist salt-crystal spalling
② Rinsing provision: periodically rinse with fresh water to remove salt → prevent concentration
③ Material upgrade: choose 316L/titanium for metal parts → resist electrochemical corrosion
④ Sealing and potting: fully pot the lead joints → isolate the brine
⑤ Salt-draining design: no stagnant pockets → salt washes away with the water
⑥ Corrosion inspection: check the coating and leads regularly → early detection
⑦ Wet-dry verification: run a salt-water wet-dry alternating test to confirm → data confirmation
⑧ Selection standardization: write intertidal-zone duty into material and protection selection → control at the source
GB/T 19746-2018 Corrosion of metals and alloys - Alternate immersion test in salt solution