E46-015 · Welding Process & Distortion · Carbon-Steel Weld · ★★
Rust and oil on the groove were not cleaned; dense porosity in the weld weakened the section and caused leakage
[Mechanism] Rust and oil decompose on heating and release hydrogen; the bubbles cannot escape in time and form porosity.
[Calculation] A porosity above 5% reduces the effective section, lowering the load capacity and causing leakage.
[Design gap] No pre-weld cleaning was carried out.
① Pre-weld cleaning: thoroughly remove rust and oil from the groove before welding to ensure a clean surface
② Dry the electrodes: dry the electrodes to specification before welding to reduce the hydrogen content
③ Control the welding speed: reduce the welding speed appropriately to help the gas escape and reduce porosity
④ Adjust the shielding-gas flow: adjust the shielding-gas flow to keep the arc stable and reduce porosity
⑤ Radiographic inspection for porosity: inspect for porosity by RT for early detection
⑥ Repair the porosity: repair the porosity defects to restore the section
⑦ Porosity verification: confirm the porosity has been eliminated by RT
⑧ Standardize process: write the pre-weld cleaning requirement into the welding procedure specification (WPS), controlling at the source
GB/T 3323-2005 Radiographic examination of fusion-welded joints in metals