E46-077 · Heat Treatment & Stress · High-Carbon Die Steel Part · ★★
A high-carbon die steel with a complex shape was oil-quenched by mistake; the cooling rate was too low to harden the core, and switching to water quenching cracked 4 pieces.
[Mechanism] Oil quenching was chosen first, but its cooling rate was too low to harden the part; switching to water quenching raised the cooling rate sharply and generated huge stresses that cracked it.
[Calculation] Water quenching cools about 5 times faster than oil quenching, so the stress exceeds the cracking limit.
[Design gap] The medium was not selected according to the shape and the material.
① Choose the right medium: select the medium by shape and material, and use interrupted or isothermal quenching for complex crack-prone parts
② Interrupted quenching: use nitrate-salt interrupted quenching to reduce stress while balancing hardness and crack resistance
③ Control the medium temperature: keep the quenching medium within the process range to stabilize the cooling rate
④ Pre-cooling: let the part cool slightly after leaving the furnace before quenching to reduce thermal stress
⑤ Crack inspection: inspect for cracks after quenching
⑥ Rework: remove the defects from cracked parts and re-process them
⑦ Quality verification: confirm acceptance by hardness testing and flaw detection
⑧ Standardize process: write the medium selection into the process card, controlling at the source
GB/T 16924-2008 Quenching and tempering of steel