E46-083 · Heat Treatment & Stress · 45 Steel Shaft · ★★★
A 45 steel shaft was medium-frequency hardened; axial cracks appeared in the transition zone between the hardened layer and the core, and the shaft broke after installation.
[Mechanism] The transition zone has a steep hardness gradient and tensile stress concentration, so cracks initiate at the boundary between the hardened layer and the soft core.
[Calculation] The high stress concentration factor in the transition zone makes the axial tensile stress exceed the strength.
[Design gap] Neither the transition-zone gradient nor the tempering was controlled.
① Gentle transition: optimize the induction parameters so the hardness transitions smoothly from the hardened layer to the core
② Timely tempering: temper promptly after quenching to lower the tensile stress in the transition zone
③ Control the frequency: select a suitable frequency so the case depth and transition zone are reasonable
④ Preheating: preheat appropriately to reduce the temperature difference between the surface and the core
⑤ Crack check: after quenching use flaw detection to check for axial cracks
⑥ Rework: remove the defects and re-quench and temper cracked shafts
⑦ Quality verification: confirm there is no cracking by flaw detection and the hardness gradient
⑧ Standardize process: write the transition control into the process card, controlling at the source
GB/T 5617-2005 Determination of effective depth of hardening after induction or flame hardening of steel