E46-090 · Heat Treatment & Stress · Cast Iron Guideway · ★★
A cast iron guideway was laser-hardened; unhardened soft bands appeared at the scan overlaps, and after wear the guideway sank 0.2mm in a wavy pattern.
[Mechanism] Improper laser scan overlap causes secondary tempering in the overlap zone, forming soft bands and uneven wear resistance.
[Calculation] The soft band is 15HRC lower than the hardened zone and wears quickly.
[Design gap] The overlap amount and scan path were not specified.
① Specify the overlap: control the laser scan overlap to avoid secondary-tempering soft bands
② Optimize the path: plan the scan path so the overlap is uniform with no gaps
③ Control the power: keep the laser power and scan speed stable to ensure hardening
④ Hardness check: after hardening measure the hardness distribution to find soft bands
⑤ Re-harden: re-scan and harden the soft band zones
⑥ Metallographic check: examine the hardened layer to confirm it is continuous
⑦ Quality verification: confirm there are no soft bands by the hardness distribution
⑧ Standardize process: write the overlap specification into the process card, controlling at the source
GB/T 18683-2002 Laser surface hardening of iron and steel parts