E46-094 · Heat Treatment & Stress · Long Shaft · ★★
A long shaft was hot-straightened after quenching and assembled without stress relief; after 3 months of operation the bend reached 0.4mm, exceeding the 0.1mm limit, and the bearing failed prematurely.
[Mechanism] Straightening introduces new plastic-deformation stress; without stress relief it releases over time and causes later bending.
[Calculation] The straightening residual stress causes later distortion four times the tolerance.
[Design gap] No stress-relief treatment was arranged after straightening.
① Stress relief after straightening: arrange stress-relief annealing after hot or cold straightening to remove the straightening stress
② Better straightening method: prefer hot-spot straightening to reduce residual stress
③ Control the straightening amount: keep the straightening amount small to avoid large plastic deformation
④ Stabilize by aging: after straightening and stress relief let the part stabilize before finish machining
⑤ Distortion monitoring: before assembly measure the straightness; if out of tolerance, re-straighten
⑥ Stress check: measure the residual stress to confirm it has dropped
⑦ Distortion verification: track the straightness over the long term to confirm stability
⑧ Standardize process: write stress relief after straightening into the process, controlling at the source
GB/T 16923-2008 Normalizing and annealing of steel