E46-097 · Heat Treatment & Stress · TC4 Titanium Alloy · ★★
A TC4 titanium alloy was annealed in an ordinary air furnace; an oxygen-rich brittle alpha layer 0.1mm thick formed on the surface, the surface cracked in the bend test, and the fatigue life dropped.
[Mechanism] Heating in an air furnace makes the titanium surface absorb oxygen and form a brittle alpha layer, reducing ductility and promoting cracking.
[Calculation] A 0.1mm alpha-brittle layer lowers the surface ductility and initiates fatigue sources.
[Design gap] Vacuum or argon-protected heating was not used.
① Vacuum or inert protection: heat-treat titanium alloys in a vacuum furnace or with argon protection to prevent oxygen pickup
② Control the furnace atmosphere: in an air furnace apply an anti-oxidation coating and limit the temperature and time
③ Remove the brittle layer: machine off the alpha-brittle layer from already oxidized parts
④ Metallographic check: inspect the surface for an oxygen-rich layer and contamination
⑤ Bend test: carry out a bend test to confirm the ductility is acceptable
⑥ Charge clean: keep the workpieces clean and free of oil to reduce contamination
⑦ Quality verification: confirm there is no alpha embrittlement by surface inspection and bend testing
⑧ Standardize process: write the protective heating into the process card, controlling at the source
GB/T 3620.1-2016 Designation and chemical composition of titanium and titanium alloys