Knowledge Base › Process and Assembly Error Case Study › Insufficient Mold Compaction Causing Swelling

Insufficient Mold Compaction Causing Swelling

E46-304 · Casting & Forging · Sand Casting · ★★

Problem Description

The mold compaction was only 65% (should be ≥80%); after pouring the mold wall bulged outward, the casting thickened locally by 3mm, and dimensions went out of tolerance.

Root Cause

[Mechanism] Insufficient compaction leaves large voids between sand grains; the static pressure of the iron displaces and expands the mold wall.
[Calculation] The mold-wall displacement grows as compaction falls; at 65% compaction the displacement is about twice that at 80%.
[Design gap] No lower compaction limit was specified and no check was made.

Corrective Solution

① Specify compaction: set a compaction lower limit of ≥80% by mold location
② Check compaction: spot-check with a compaction tester and re-ram if below the lower limit
③ Control the molding sand: mix per the recipe to ensure green strength
④ Ram evenly: compact uniformly by hand or machine, avoiding uneven density
⑤ Dimension check: open the flask and measure the casting wall thickness, detecting swelling early
⑥ Die verification: check that the pattern dimensions are correct
⑦ Swelling verification: confirm compliance by dimension measurement
⑧ Standardize process: write the compaction requirements into the work instruction, controlling at the source

Checklist

Reference

GB/T 9442-2010 Silica Sand for Foundry Use

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »