E46-310 · Casting & Forging · Machine-Bed Casting · ★★★
Before aging, a machine-bed casting distorted 2mm in overall length; the flatness of the guideway surface was out of tolerance by 0.3mm, and it warped after machining.
[Mechanism] Uneven cooling of the casting's sections produces thermal and transformation stresses; the release of residual stress causes distortion.
[Calculation] A large wall-thickness difference leads to a difference in cooling rate, and residual stress grows as the wall-thickness difference increases.
[Design gap] No annealing or natural aging was set up to relieve stress.
① Stress-relief annealing: anneal promptly after casting to relieve residual stress
② Natural aging: when annealing is not available, leave the part outdoors long enough
③ Uniform wall thickness: design for as uniform a thickness as possible to reduce the cooling difference
④ Symmetric structure: use symmetric sections to reduce the warping tendency
⑤ Distortion measurement: measure distortion before and after rough machining, detecting problems early
⑥ Repeat aging: age again between rough and finish machining to stabilize dimensions
⑦ Distortion verification: confirm flatness by CMM
⑧ Standardize process: write the aging step into the process route, controlling at the source
JB/T 50164-2016 Heat treatment specifications for iron castings