E46-314 · Casting & Forging · Cast Steel Part · ★★★
A cast steel part developed hot tears at the corners and hot spots, 20 to 50mm long; the cracks were oxidized, and magnetic particle inspection showed a network pattern.
[Mechanism] At the end of solidification the liquid film at the grain boundaries is weak; restricted linear contraction causes hot tearing.
[Calculation] The hot-tearing tendency rises with sulfur and phosphorus segregation and linear contraction; cracks initiate in the temperature range where strength is lowest.
[Design gap] Sulfur and phosphorus and the corner fillets were not controlled.
① Control sulfur and phosphorus: limit their content in the molten steel to lower the hot-tearing tendency
② Use fillets: use generous fillets at internal corners to reduce stress concentration
③ Reduce restraint: optimize the gating/risering and core irons to reduce contraction restraint
④ Cut linear contraction: adjust the composition and temperature to reduce linear contraction
⑤ Crack check: magnetic particle inspect the hot spots and corners, detecting problems early
⑥ Slow cooling: cool slowly after shakeout to reduce stress
⑦ Crack verification: confirm the absence of hot tears by inspection
⑧ Standardize process: write the sulfur/phosphorus limits and fillets into the drawings, controlling at the source
GB/T 11352-2009 Cast carbon steel castings for general engineering use