E46-316 · Casting & Forging · Sand Casting · ★★
Sand holes were dense on the surface and inside the casting, up to 5mm; the holes were exposed after machining and tightness dropped.
[Mechanism] Molding or core sand is eroded and drawn into the iron, or the mold sand spalls off because its strength is insufficient, forming sand holes.
[Calculation] The erosion increases with the square of the flow velocity; the number of sand holes rises with erosion and insufficient strength.
[Design gap] Sand erosion and molding sand strength were not controlled.
① Increase strength: control the green and dry strength of the molding sand by location
② Provide sand traps: fit sand-collecting wells and screens in the runner to trap sand
③ Fill with steady flow: control the pouring rate to reduce erosion
④ Case the surface: brush a coating on the mold cavity to improve erosion resistance when necessary
⑤ Sand hole check: check the machined surface and use X-ray for sand holes, detecting problems early
⑥ Tightness test: run a leak or flaw-detection test to confirm
⑦ Sand hole verification: confirm the absence of out-of-limit sand holes by testing
⑧ Standardize process: write the sand strength and runner design into the work instruction, controlling at the source
GB/T 9442-2010 Silica Sand for Foundry Use