Knowledge Base › Process and Assembly Error Case Study › Lost Foam Coating Defect Causing Sand Burn-On

Lost Foam Coating Defect Causing Sand Burn-On

E46-319 · Casting & Forging · Lost Foam Casting · ★★

Problem Description

A lost foam casting had sand burn-on and a pitted surface; where the coating layer peeled off the surface was rough and out of tolerance, making sand removal difficult.

Root Cause

[Mechanism] Poor coating permeability or an uneven coating traps the pyrolysis gas from the pattern; the metal penetrates the coating and forms burn-on.
[Calculation] A coating permeability below the critical value raises the back pressure, and metal penetration increases with the back pressure.
[Design gap] Coating permeability and coating thickness were not controlled.

Corrective Solution

① Choose the coating: use a high-permeability coating made for lost foam
② Control thickness: brush the coating evenly to the specified thickness with no misses
③ Dry thoroughly: fully dry the coating to remove moisture
④ Compact the flask: vibrate the dry sand tight with no voids
⑤ Surface check: open the flask and check for burn-on and pitting, detecting problems early
⑥ Sand-removal confirmation: check the roughness after sand removal
⑦ Coating verification: confirm the absence of burn-on by surface quality
⑧ Standardize process: write the coating specification into the work instruction, controlling at the source

Checklist

Reference

GB/T 35382-2017 Lost Foam Casting - Coatings