E46-320 · Casting & Forging · Die Casting · ★★
The corners and far ends of the die casting were misrun with missing metal; the thinnest point was only 0.6mm thick (should be 1.5mm), and the contour was unclear.
[Mechanism] Insufficient injection velocity or specific pressure leaves the far end of the cavity unfilled before the metal solidifies.
[Calculation] A filling pressure below the critical value leaves insufficient flow velocity at the far end; misrun increases with thinner walls and longer flow paths.
[Design gap] The injection parameters and overflow/venting were not checked.
① Increase the specific pressure: raise the injection specific pressure by wall thickness to ensure filling
② Add overflow: place overflow and vent grooves at the far end to discharge dross and gas
③ Control velocity: optimize the injection velocity profile (slow-fast-slow)
④ Die temperature control: keep the die working temperature uniform
⑤ Misrun check: open the die and check the contour filling, detecting problems early
⑥ Adjust the process: raise the pouring temperature when necessary
⑦ Fill verification: confirm the absence of missing metal by the contour
⑧ Standardize process: write the injection parameters into the process card, controlling at the source
GB/T 15114-2009 Aluminum Alloy Die Castings