Knowledge Base › Process and Assembly Error Case Study › Forging Temperature Too High Causing Overheating

Forging Temperature Too High Causing Overheating

E46-323 · Casting & Forging · Alloy Steel Forging · ★★★

Problem Description

An alloy steel forging was heated to 1280℃ (should be 1150℃); the post-forging grain size reached grade 5 (should be ≥8), and toughness dropped.

Root Cause

[Mechanism] Overheating grows the austenite grains; the coarse grains retained after forging reduce toughness.
[Calculation] Grains grow with heating temperature and time; exceeding the temperature coarsens the grain size exponentially.
[Design gap] The upper heating limit and holding time were not controlled.

Corrective Solution

① Control the upper heating limit: set the maximum heating temperature by steel grade
② Control the holding time: limit the high-temperature hold to prevent coarsening
③ Temperature monitoring: control temperature in real time with thermocouples
④ Normalizing: re-normalize overheated parts to refine the grains
⑤ Grain size check: sample and check the grain size after forging, detecting problems early
⑥ Toughness check: run impact tests when necessary
⑦ Grain verification: confirm compliance by grain size
⑧ Standardize process: write the heating temperature into the heating specification, controlling at the source

Checklist

Reference

GB/T 13320-2007 Steel die forgings - Grain size