Uneven Die Temperature in Die Casting

E46-344 · Casting & Forging · Die Casting · ★★

Problem Description

A die casting had localized cold shuts and shrinkage depressions; the die temperature varied by as much as 80℃ and part quality fluctuated within the same die.

Root Cause

[Mechanism] Unevenly arranged cooling channels make the die temperature vary widely, causing poor local filling or shrinkage depressions.
[Calculation] A die temperature difference causes local cooling-rate variation; cold shuts grow with the difference and shrinkage depressions with local overheating.
[Design gap] The cooling channels were not arranged evenly.

Corrective Solution

① Even channel layout: lay out cooling channels evenly according to hot spots
② Control die temperature: use a die temperature controller to keep working temperature even
③ Measure die temperature: use multi-point measurement to monitor the temperature difference
④ Adjust spraying: spray more locally to reduce uneven temperature
⑤ Check for defects: inspect for cold shuts and shrinkage depressions on mold opening, detecting problems early
⑥ Adjust the process: balance the die temperature and re-cast
⑦ Die temperature verification: confirm evenness by part quality
⑧ Standardize process: write the channel layout into the die drawing, controlling at the source

Checklist

Reference

GB/T 15114-2009 Aluminum Alloy Die Castings