Knowledge Base › Process and Assembly Error Case Study › Investment Casting Shell Cracking

Investment Casting Shell Cracking

E46-345 · Casting & Forging · Investment Casting · ★★★

Problem Description

During dewaxing or pouring, the investment casting shell cracked; the casting flashed and suffered short-run and distortion.

Root Cause

[Mechanism] Insufficient shell strength or too-fast dewaxing creates a pressure difference across the shell and cracks it.
[Calculation] Shell strength falls as the number of coating layers decreases, and a dewaxing heating rate above the critical value cracks it.
[Design gap] The number of coating layers and the dewaxing rate were not controlled.

Corrective Solution

① Add coating layers: ensure sufficient shell layers and firing
② Control dewaxing: keep the heating rate steady in steam dewaxing
③ Fire fully: fire the shell thoroughly to remove wax and strengthen it
④ Support the shell: support the shell during pouring to prevent distortion
⑤ Check for shell cracks: inspect shell integrity before pouring, detecting problems early
⑥ Adjust the process: reinforce or remake the shell
⑦ Shell strength verification: confirm crack-free pouring
⑧ Standardize process: write the shell-making specification into the process card, controlling at the source

Checklist

Reference

GB/T 38431-2019 Investment casting - Process

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL