Knowledge Base › Process and Assembly Error Case Study › Insufficient Preheating of Permanent Molds Causing Cracking

Insufficient Preheating of Permanent Molds Causing Cracking

E46-346 · Casting & Forging · Permanent Mold Casting · ★★

Problem Description

The first article from permanent mold casting cracked by chill; the mold temperature was only 80℃ (should be 200℃) and the casting surface was crazed.

Root Cause

[Mechanism] A metal mold conducts heat quickly; insufficient preheating chills the casting, and the stress between surface and core causes cracking.
[Calculation] Below the critical mold temperature the cooling rate rises sharply, and cracking grows with the temperature difference.
[Design gap] The permanent mold was not preheated to working temperature.

Corrective Solution

① Preheat the mold: preheat the permanent mold above 200℃ to working temperature
② Control mold temperature: keep the mold temperature even during casting
③ Apply coating: brush insulating coating on the mold cavity to buffer
④ Control pouring: use adequate temperature to reduce chill
⑤ Check for cracks: inspect for crazing when the mold opens, detecting problems early
⑥ Adjust the process: raise the mold temperature and recast
⑦ Mold temperature verification: confirm crack-free filling
⑧ Standardize process: write the mold preheating into the process card, controlling at the source

Checklist

Reference

GB/T 9438-2013 Aluminum-alloy castings