Knowledge Base › Process and Assembly Error Case Study › Improper Casting Fillets Causing Stress Cracks

Improper Casting Fillets Causing Stress Cracks

E46-347 · Casting & Forging · Casting · ★★

Problem Description

A casting had a sharp square internal corner; it cracked where solidification stresses concentrated, and magnetic particle inspection revealed cracks at the corner.

Root Cause

[Mechanism] A sharp internal corner gives a high stress concentration factor, and solidification shrinkage stress exceeds the strength to cause cracking.
[Calculation] Stress concentration rises as the fillet radius shrinks; a sharp corner carries several times the stress of an R5 fillet.
[Design gap] An adequate fillet was not provided at the internal corner.

Corrective Solution

① Provide fillets: use an adequate fillet radius at internal corners
② Optimize structure: avoid abrupt wall-thickness changes by providing transitions
③ Reduce restraint: arrange gates and risers so they do not restrain shrinkage there
④ Slow-cool the corner: slow-cool the corner to reduce stress
⑤ Check for cracks: magnetic particle inspect the internal corner, detecting problems early
⑥ Stress measurement: measure residual stress when necessary
⑦ Fillet verification: confirm the absence of cracks by inspection
⑧ Standardize process: write the fillet into the drawing, controlling at the source

Checklist

Reference

GB/T 6414-2017 Castings - Dimensional tolerances