Investment Casting Dimension Out of Tolerance

E46-350 · Casting & Forging · Investment-Cast Part · ★★

Problem Description

An investment-cast part was out of tolerance by 0.4mm (should be 0.2mm), as wax pattern shrinkage and shell expansion combined to cause the deviation.

Root Cause

[Mechanism] Fluctuations in wax pattern shrinkage and shell expansion combine to shift the final dimension.
[Calculation] The total deviation is the algebraic sum of wax shrinkage and shell expansion; exceeding the tolerance requires die compensation.
[Design gap] Shrinkage was not measured to compensate the die.

Corrective Solution

① Measure shrinkage: measure the actual wax pattern and alloy shrinkage rates
② Die compensation: scale up the die dimensions according to the shrinkage rate
③ Control the shell: stabilize the shell expansion rate
④ Control pouring temperature: stabilize the pouring temperature to reduce variation
⑤ Check dimensions: measure the first article on a CMM, detecting problems early
⑥ Adjust the die: modify the die to compensate where out of tolerance
⑦ Dimension verification: confirm compliance on a CMM
⑧ Standardize process: write the shrinkage compensation into the die drawing, controlling at the source

Checklist

Reference

GB/T 38431-2019 Investment casting - Process