E46-355 · Surface Treatment & Coating · Vertical Panel · ★
After spraying, a vertical panel showed sagging tear marks near the bottom; the wet film locally exceeded 300μm (should be 120μm), giving an uneven appearance and film thickness.
[Mechanism] A high single-pass paint output with a slow gun traverse makes the wet film too thick, causing gravity sagging.
[Calculation] A wet film above 200μm exceeds the critical sagging thickness, and the critical value is even lower on vertical surfaces.
[Design gap] Gun traverse speed and paint output were not limited.
① Limit traverse speed: keep the gun at a uniform 0.3 m/s to avoid paint buildup
② Control paint output: adjust the gun output for a 120μm single-pass wet film
③ Multiple thin coats: build up with several thin passes to reduce sagging
④ Check for sagging: monitor the vertical-surface critical limit during application, detecting problems early
⑤ Sand smooth: once dry, sand the sagged areas and respray to restore a flat finish
⑥ Adjust viscosity: set the thinner ratio according to temperature and humidity to keep atomization stable
⑦ Appearance verification: confirm evenness by visual inspection and film thickness, verified by data
⑧ Standardize process: write the gun traverse parameters into the spraying specification, controlling at the source
GB/T 30790.1-2014 Paints and varnishes - Protective coating systems