E46-357 · Surface Treatment & Coating · Powder-Coated Part · ★★
After curing, a powder-coated part had a tacky surface and failed on impact; the oven temperature was 160℃ (should be 200℃) with too short a dwell, leaving the resin under-crosslinked.
[Mechanism] A low curing temperature and short time leave the resin insufficiently crosslinked, making the coating soft and brittle.
[Calculation] Epoxy powder should be held at 200℃ for 10 min; every 10℃ drop lowers the degree of crosslinking by about 15%.
[Design gap] The oven temperature was not measured against the conveyor speed.
① Measure oven temperature: use a temperature profiler to record the actual part temperature and control the profile
② Control temperature: hold the curing oven stable at 200℃ to ensure crosslinking
③ Control conveyor speed: set it per oven length to give 10 min for full curing
④ Check hardness: use the pencil hardness test to verify ≥H, detecting problems early
⑤ Re-cure: return under-cured parts to the oven to restore properties
⑥ Control pretreatment: ensure the phosphating is sound before powder application to preserve adhesion
⑦ Performance verification: confirm compliance by impact and hardness tests, verified by data
⑧ Standardize process: write the curing profile into the powder procedure, controlling at the source
GB/T 21782.1-2008 Coating powders - Part 1