Knowledge Base › Process and Assembly Error Case Study › Poor Screen-Printing Adhesion, Missing Characters

Poor Screen-Printing Adhesion, Missing Characters

E46-369 · Surface Treatment & Coating · Equipment nameplate · ★

Problem Description

The screen-printed characters on the equipment nameplate could be wiped off by hand; the ink was not cured or the substrate was untreated, so adhesion was poor.

Root Cause

[Mechanism] Oil on the substrate or insufficiently cured ink leaves a weak interface bond, so the characters come off.
[Calculation] Uncured ink has adhesion below 0.3MPa, versus 2MPa after curing.
[Design gap] Substrate cleaning and cure confirmation were not performed.

Corrective Solution

① Clean the substrate: degrease cleanly before screen printing to ensure bonding
② Control curing: choose UV or oven curing according to the ink and cure fully for durability
③ Choose ink: select ink matched to the substrate to improve adhesion
④ Adhesion check: use the tape test to check for no character loss and detect problems early
⑤ Reprint: clean and reprint parts with missing characters to restore legibility
⑥ Control film thickness: keep the ink thickness moderate to prevent build-up and cracking
⑦ Adhesion verification: confirm firmness by tape testing, confirmed by data
⑧ Standardize process: write cleaning and curing into the screen-printing process, controlling at the source

Checklist

Reference

GB/T 20521-2006 Screen printing - General technical requirements