E46-442 · Commissioning & Run-In · Plain bearing · ★★★
The plain bearing's assembly clearance was set at the lower limit; after the run-in temperature rose, the shaft expanded and seized, and the sudden temperature spike tripped the shutdown.
[Mechanism] The clearance is smaller than the thermal expansion, so the journal grows tight once the temperature rises.
[Calculation] A 60 K temperature rise expands the journal by more than 0.05mm; with insufficient clearance it seizes.
[Design gap] No clearance for thermal expansion was provided.
① Leave clearance: set the assembly clearance at the middle-to-upper limit, allowing for thermal expansion
② Calculate expansion: compute the journal expansion from the temperature rise and confirm the clearance is sufficient
③ Slow warm-up: raise the temperature slowly during run-in and watch the temperature curve
④ Measure temperature: reduce speed once it exceeds 85℃, preventing seizure
⑤ Re-measure: re-measure the clearance in the hot state to confirm there is no binding
⑥ Record: record the clearance and the temperature rise
⑦ Quality verification: confirm acceptance by no seizure in the hot state, confirmed by data
⑧ Standardize process: write the upper clearance limit into the assembly card, controlling at the source
GB/T 10445-2008 Plain bearings - Hydrodynamic plain journal bearings under steady-state conditions