E46-453 · Dimension Chain & Tolerance Coordination · Turbocharger · ★★★
The turbocharger rotor-to-housing cold clearance was 0.30 mm, but at the 600℃ working temperature the measured thermal elongation made the clearance -0.05 mm, and the rotor rubbed the housing and seized.
[Mechanism] The shaft and housing have different coefficients of linear expansion, so after heating their elongations differ and the fit clearance shrinks to negative.
[Calculation] Elongation ΔL=αLΔT; steel α=12×10⁻⁶/℃, L=120 mm, ΔT=580℃, ΔL=0.83 mm, clearance 0.30-0.83 < 0.
[Design gap] No thermal dimension chain calculation was done, and the cold clearance left no thermal compensation.
① Calculate expansion: check the thermal elongation of each part at working temperature, controlling at the source
② Leave clearance: reserve thermal elongation in the cold state so the hot clearance is a positive 0.10 mm, confirmed by data
③ Select material: match the coefficients of linear expansion to reduce the difference, detecting problems early
④ Measure temperature: measure the actual working temperature before computing clearance, preventing seizure
⑤ Compensate: provide an expansion joint or clearance-adjusting structure, ensuring no hot-state rubbing
⑥ Verify clearance: measured hot-state clearance ≥0.05 mm, correcting early
⑦ Quality verification: confirm no seizure by hot-state clearance, confirmed by data
⑧ Standardize process: write the thermal dimension chain into the thermal design check, controlling at the source
GB/T 1800.2-2020 Geometrical product specifications (GPS) - Linear size tolerances