Design Fundamentals · Material Selection (Quick Reference)

Basic Principles of Material Selection

【General Principles of Material Selection】

① Service performance requirements (strength / hardness / wear resistance / corrosion resistance / heat resistance)

② Process performance requirements (castability / forgeability / weldability / machinability / heat-treatability)

③ Economic requirements (material cost + machining cost + heat treatment cost)

④ Availability (market supply / delivery lead time)

【Selection Guide for Common Materials】

Shaft parts: C45 steel (light load), 40Cr (medium load), 20CrMnTi (heavy load)

Gears: C45 steel quenched and tempered (low speed), 40Cr quenched and tempered (medium speed), 20CrMnTi carburized (high speed)

Housings / casings: HT250 (general), QT500 (high strength), ZL102 (lightweight)

Springs: 65Mn (general), 50CrVA (high fatigue resistance)

Wear parts: GCr15 (bearings), Cr12MoV (dies)

【Common Misconceptions in Material Selection】

① Higher strength is not always better - toughness must also be considered

② High-alloy steel is not necessarily better than carbon steel - process complexity matters

③ Do not overlook the supply channel - special materials may require a six-month procurement cycle

④ Heat treatment is the key to realising material properties - consider heat-treatability when selecting material

【Cost Reference】

Plain carbon steel: about 3~5 CNY/kg

Alloy steel: about 5~8 CNY/kg

Stainless steel: about 15~30 CNY/kg

Aluminium alloy: about 20~40 CNY/kg

General Rules for Selecting Materials for Machine Parts

【Material Selection Principles for Parts】

① Load level: general parts → 45 steel / critical parts → 40Cr / high strength → 42CrMo

② Working temperature: <120℃ → general steel / <300℃ → heat-resistant steel / >500℃ → superalloy

③ Wear resistance requirement: general → quenched and tempered / medium-high → quenched / high → carburized or nitrided

④ Corrosive environment: water → stainless steel 304 / acid → 316L / seawater → duplex stainless steel

⑤ Weight requirement: weight reduction → aluminium alloy / ultra-light → magnesium alloy or carbon fibre

⑥ Cost: large batch → castings (HT250) / small batch → welded (Q235)

Comparison of 45 Steel and 40Cr

【45 Steel vs 40Cr Selection】

45 steel:

• Low price (about 6~8 CNY/kg)

• Quenched and tempered HB220~250 / σb≈650MPa

• Average hardenability (critical diameter about 12mm)

• Suitable for unimportant general shafts and gears

40Cr:

• Slightly higher price (about 10~14 CNY/kg)

• Quenched and tempered HB240~285 / σb≈980MPa

• Better hardenability (critical diameter about 25mm)

• Suitable for critical shafts and gears

Conclusion: use 40Cr for critical parts with a section larger than 20mm

Comparison of Cast Iron and Cast Steel

【Cast Iron vs Cast Steel Selection】

Grey cast iron HT250:

• Compressive >750MPa / tensile about 250MPa

• Good vibration damping (2~3 times that of steel)

• Good fluidity (suitable for complex parts)

• Lowest price (about 5~8 CNY/kg)

• Suitable for: housings / machine tool beds / bases

Cast steel ZG270-500:

• Tensile about 500MPa (isotropic)

• Good weldability

• Suitable for: impact-loaded castings / welded parts

• Higher price (about 12~18 CNY/kg)

Related quick references: Tolerances & FitsSurface RoughnessMaterial Heat TreatmentCast Part DesignGeometrical TolerancesDimension ChainsWelded StructuresSheet Metal StructuresShafting DesignSeal DesignHeat TreatmentDatum ReferencingTolerance Principles

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL