Design Fundamentals · Heat Treatment (Quick Reference)

Guide to Heat Treatment Process Selection

【Normalizing】

Purpose: refine grain size, relieve internal stress, improve machinability

Applicable materials: medium-carbon steel, low-carbon steel

Features: simple process, low cost

【Annealing】

Purpose: reduce hardness, relieve internal stress, refine the structure

Applicable to: high-carbon steel, alloy steel (spheroidizing anneal)

【Quenched and Tempered】(quenching + high-temperature tempering)

Purpose: obtain good overall mechanical properties (strength + toughness)

Applicable to: heavily loaded structural parts (shafts / gears / connecting rods)

Hardness: HB 200~300

【Quenching + Low-temperature Tempering】

Purpose: obtain high hardness and high wear resistance

Applicable to: cutting tools, dies, wear parts

Hardness: HRC 48~62

【Carburizing and Quenching】

Purpose: high surface hardness + high core toughness

Applicable materials: low-carbon steel (such as 20CrMnTi)

Carburized case depth: 0.5~1.5mm

Applications: heavy-duty gears, transmission shafts

【Nitriding】

Purpose: ultra-high surface hardness, high wear resistance, corrosion resistance

Applicable materials: steels containing Al/Cr (such as 38CrMoAl)

Nitrided case depth: 0.3~0.6mm

Features: minimal distortion, can be nitrided in the finished condition

Applications: precision spindles, dies

Quenched and Tempered Treatment (Quenching + High-temperature Tempering)

【Quenched and Tempered Process】

Process: quenching (820~860℃) → high-temperature tempering (550~650℃)

Purpose: obtain a tempered sorbite structure → excellent overall mechanical properties

Typical parameters:

45 steel: quench 840℃ water cooling + temper 580℃ → HB220~250

40Cr: quench 850℃ oil cooling + temper 570℃ → HB240~285

42CrMo: quench 850℃ oil cooling + temper 560℃ → HB280~340

Note: with a large section the cooling is insufficient → the core hardness falls below the surface hardness

Selection of Quenching Media

【Quenching Media Selection】

Water (most commonly used):

• Fast cooling (800~400℃ / about 150℃/s)

• Forms a vapour film (affects uniformity)

• Prone to quench cracking (suitable for carbon steel / T10 / W18Cr4V)

• Water temperature must be <30℃

Oil (quenching oil / machine oil):

• Slower cooling (about 20~60℃/s)

• Uniform cooling

• Not prone to quench cracking

• Suitable for alloy steels (40Cr / GCr15)

Brine / caustic solution:

• Fastest cooling (no vapour film / uniform)

• Used for steels of low hardenability

Relation Between Tempering Temperature and Hardness (45 Steel)

【45 Steel Tempering Temperature vs Hardness】

150~200℃→HRC55~50 (low-temperature tempering / high hardness)

200~350℃→HRC50~45 (medium-temperature tempering / for springs)

350~500℃→HRC45~35 (medium-to-high temperature tempering)

500~650℃→HRC35~20 (high-temperature tempering / quenched and tempered)

Principle: the higher the hardness requirement → the lower the tempering temperature

But 200~350℃ is the temper embrittlement zone (avoid tempering in this range)

Quenched and tempered recommendation: temper at 540~580℃ (giving HB220~250, the best overall properties)

Carburizing Process Parameters

【Carburizing Process】

Purpose: raise the surface hardness of low-carbon steel (20Cr / 20CrMnTi)

Parameters:

• Carburizing temperature: 880~940℃ (gas carburizing)

• Time: according to the required case depth (0.2mm/h)

• Case depth: 0.5~2mm

• Surface carbon content: 0.8~1.0%

• Quenching: direct quenching / reheat and quench

• Tempering: 160~200℃

Result: surface HRC58~63 / core HRC35~45

Applications: gears / cams / shafts

Related quick references: Tolerances & FitsSurface RoughnessMaterial Heat TreatmentCast Part DesignGeometrical TolerancesDimension ChainsWelded StructuresSheet Metal StructuresShafting DesignSeal DesignMaterial SelectionDatum ReferencingTolerance Principles