S-N Curve and Fatigue Limit

[S-N Curve (sigma-N curve)]

σ^m·N = C

m — material constant (steel 3~9, non-ferrous 3~5)

C — constant

Or written as:

σ = σD·(ND/N)^(1/m)

sigma_D — reference fatigue strength

N_D — cycles corresponding to sigma_D

[Fatigue Limit (endurance limit)]

Horizontal segment after N >= N0 (steel N0 approx 10^7)

sigma_-1 — fully reversed fatigue limit (MPa)

[Empirical sigma_-1 Estimate]

Steel: sigma_-1 approx 0.40~0.50 dot sigma_b

σ-1 ≈ 0.27(σb+σs)

Cast iron: sigma_-1 approx 0.40 dot sigma_b

Aluminum: sigma_-1 approx 0.30~0.40 dot sigma_b

Copper alloy: sigma_-1 approx 0.30~0.40 dot sigma_b

[Typical Material Fatigue Limits]

45 steel (Q&T): sigma_b = 700, sigma_-1 = 300~350

40Cr (Q&T): sigma_b = 900, sigma_-1 = 400~450

20CrMnTi (carburized): sigma_-1 = 550~650

60Si2Mn (spring): sigma_-1 = 600~700

HT250:σ-1=100~120

ZL102:σ-1=60~80

[Factors Affecting Fatigue Limit]

(1) Surface condition

Polished 1.0, ground 0.95, fine-turned 0.85, rough-turned 0.75, forged 0.55

(2) Size (size effect)

Large specimen sigma_-1 lower (more weak points)

d=10mm: β=1.0

d=50mm: β=0.85

d=100mm: β=0.75

(3) Surface strengthening

Induction hardening 1.5~2.0

Carburizing 1.5~2.0

Shot peening 1.3~1.5

Rolling 1.3~1.5

(4) Stress concentration

Kf = 1 + q(Kt - 1), q sensitivity (0.5~0.9)

[Unsymmetrical Cycle Fatigue]

Finite life region (10^4 < N < 10^7):

σa = σ-1·(1 - σm/σb)^m

Or Gerber formula:

σa = σ-1·(1 - (σm/σb)²)

Or Goodman line (conservative):

σa = σ-1·(1 - σm/σb)

sigma_m — mean stress

sigma_a — stress amplitude

[Design Points]

(1) Steel N > 10^7 can be designed for infinite life

(2) Aluminum has no clear fatigue limit, use finite life

(3) Reducing stress concentration is most effective for fatigue life

(4) Surface strengthening is significant

Miner Linear Cumulative Damage Theory

[Miner Linear Cumulative Damage Rule]

D = Σ(ni/Ni) ≤ 1

ni — cycles at stress sigma_i

Ni — fatigue life at sigma_i (from S-N)

D — damage

Fatigue failure when D = 1

[Variable-Amplitude Life Estimate]

Given load spectrum, estimate life N:

N = 1/Σ(αi/Ni)

alpha_i — fraction of total cycles at level i

[Calculation Example]

A part load spectrum:

σ1=200MPa, n1=10⁴, N1=10⁵, D1=0.1

σ2=250MPa, n2=10³, N2=2×10⁴, D2=0.05

σ3=300MPa, n3=10², N3=5×10³, D3=0.02

Damage per block D = 0.17

Total cycles per block n_block = 11100

Total life N_total = 1/0.17 x 11100 = 65294 cycles

[Limitations of Miner Rule]

(1) Ignores load sequence

Reality: high->low overload may delay crack growth (residual compressive)

Low->high may accelerate damage

(2) Ignores underload effect

sigma < sigma_-1 theoretically Ni = infinity, but actual damage occurs

(3) Not for random loads with prominent overload peaks

[Modified Miner Rule]

(1) Modified Miner: D = Sigma(ni/Ni) <= a (a = 0.3~1.0, test value)

(2) Relative Miner: correction from similar spectrum tests

(3) Bilinear damage rule: two-stage accumulation

[Applications]

(1) Automotive part load-spectrum life prediction

(2) Wind-turbine blade fatigue design

(3) Aircraft spectrum-load life

(4) Bridge fatigue life assessment

[Load Spectrum]

(1) Rainflow counting extracts cycles

(2) Classify by amplitude and count

(3) Each ni, get Ni from S-N

(4) Miner accumulation

[Engineering Advice]

Critical parts take D <= 0.5 (conservative)

General parts take D <= 1.0

Periodic inspection (especially after D > 0.5)

Goodman Diagram and Fatigue Design Diagram

[Haigh Diagram (sigma_a - sigma_m coordinates)]

Horizontal axis sigma_m (mean stress), vertical sigma_a (amplitude)

Curve shows safe boundary of sigma_a vs sigma_m

[Goodman Line (conservative)]

σa = σ-1·(1 - σm/σb)

[Gerber Parabola]

σa = σ-1·(1 - (σm/σb)²)

[Soderberg Line (most conservative)]

σa = σ-1·(1 - σm/σs)

[Morrow Formula]

σa = (σf - σm)·(2Nf)^b

sigma_f — fatigue strength coefficient

b — fatigue strength exponent

[Fatigue Safety Factor]

n = σ-1/(σa·Kf + ψσ·σm)

psi_sigma — mean-stress influence coefficient

ψσ = σ-1/σb(Goodman)

psi_sigma = 0.1~0.2 (steel, empirical)

[Unsymmetrical Cycle Fatigue Limit]

σr = σm + σa ≤ [σ]

r = sigma_min / sigma_max stress ratio

r = -1: fully reversed, sigma_m = 0

r = 0: pulsating, sigma_m = sigma_a = sigma_max/2

r = +1: static, sigma_a = 0

[Simplify Fatigue Limit by r]

σr = σ-1·(1 + ψσ·(1+r)/(1-r))

[Calculation Example]

sigma_b = 600, sigma_-1 = 240, r = 0 (pulsating)

ψσ = 0.2

σ0 = 240·(1+0.2×(1+0)/(1-0)) = 240×1.2 = 288MPa

Practical sigma_0 approx (1.3~1.5) sigma_-1

[Applications]

(1) Complex-load fatigue design

(2) Check with sigma_a, sigma_m combination

(3) Determine safe working region

[Design Points]

(1) Mean stress up -> allowable amplitude down

(2) Compressive mean stress improves fatigue (shot peening / pre-compression)

(3) Combined stress: convert to equivalent then S-N

(4) Critical parts n >= 2, general n >= 1.5

Other quick references in this series:Mechanics FundamentalsFluid MechanicsVibrationThermodynamicsElectrical FundamentalsQuick-Calc FormulasHydraulics / Inertia CalculationGear StrengthShaft StrengthKeyed ConnectionsSpringsBolt StrengthWeld StrengthBeam and Plate Bending

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL