Design Fundamentals · Standard Data (Quick Reference)

Reference Cutting Speeds (Turning)

High speed steel tools: carbon steel 20~30m/min, alloy steel 15~25, cast iron 15~20, aluminium alloy 100~200

Cemented carbide tools: carbon steel 80~150m/min, alloy steel 60~120, cast iron 60~100, aluminium alloy 200~400

When selecting, consider the tool material / workpiece hardness / depth of cut.

Reference Cutting Speeds (Milling)

High speed steel: 20~40m/min

Cemented carbide: 80~180m/min

Coated carbide: 150~350m/min

Take the lower limit for rough milling and the upper limit for finish milling.

Reference Cutting Speeds (Drilling)

High speed steel drills: steel 15~25m/min, cast iron 20~30, aluminium alloy 50~80

Cemented carbide drills: steel 60~120m/min

Feed rate: 0.05~0.3mm/r (according to hole diameter)

Reference Cutting Speeds (Grinding)

Wheel peripheral speed: 35m/s (ordinary), 45~60m/s (high speed)

Workpiece speed: 10~30m/min

Grinding depth: rough grinding 0.02~0.05mm, finish grinding 0.005~0.01mm

Tap Drill Diameters

M3-φ2.5/M4-φ3.3/M5-φ4.2/M6-φ5.0/M8-φ6.8/M10-φ8.5/M12-φ10.3/M14-φ12.0/M16-φ14.0/M18-φ15.5/M20-φ17.5

(Applicable to steel; for cast iron / aluminium alloy the tap drill should be 0.1mm larger)

Recommended Shaft Tolerances for Bearing Fits

Deep groove ball bearing shaft fit (rotating load): for a journal φ<50mm select k6, for φ50~100 select k6/m6

Stationary load: select g6/h6

Angular contact bearings: for a shaft diameter <50 select k6/j6, >50 select m6

Taper bore bearings: select h7/js6

Recommended Bore Tolerances for Bearing Fits

Deep groove ball bearing bore fit (rotating outer ring): H7

Stationary outer ring: J7/JS7

Use H7 when the housing material is cast iron, N7 when it is aluminium alloy

The choice of tolerance zone must consider thermal expansion and the tightness of the fit.

Surface Roughness for Sealing Surfaces

Rotary shaft oil seal: Ra≤0.4μm

O-ring groove: bottom face Ra≤1.6μm, flank Ra≤3.2μm

Static sealing faces: Ra≤1.6μm

Reciprocating seals: Ra≤0.4μm (rod), Ra≤0.8μm (bore)

Spark Test Identification of Steels

Low-carbon steel: long sparks, pale yellow colour, few bursts

Medium-carbon steel: brighter sparks, more bursts

High-carbon steel: short dense sparks, many bursts

High-speed steel: dark red sparks, no bursts

Chrome steel: white sparks, star-shaped bursts

Casting Shrinkage Rates

Grey cast iron: 0.7~1.0%

Ductile iron: 0.8~1.2%

Cast steel: 1.5~2.0%

Aluminium alloy: 1.0~1.3%

Copper alloy: 1.2~1.8%

The shrinkage rate must be taken into account when designing the pattern.

Reference Forging Ratios

Carbon structural steel: 2~3

Alloy structural steel: 3~4

Stainless steel: 3~5

Tool steel: 5~10

An insufficient forging ratio gives inadequate structure density and poor mechanical properties.

Welding Preheat Temperatures

Q235 (<20mm): no preheat

Q235 (20~40mm): 50~100℃

45 steel: 100~200℃

40Cr: 200~300℃

Stainless steel: no preheat (keep the interpass temperature <150℃)

Preheating reduces the cooling rate and prevents cold cracking.

Estimating Heat Treatment Heating Time

Heating time = K×D (min)

K — heating coefficient: box furnace 1.0~1.5, salt bath furnace 0.5~1.0

D — effective thickness of the workpiece (mm)

Tempering holding time = quenching holding time × 1.5~2.0

Large-section workpieces need a proportionally longer time.

Reference Grinding Wheel Selection

Grinding 45 steel: white alumina WA46~60K~L

Grinding 40Cr: white alumina WA46~60K~L

Grinding cemented carbide: green silicon carbide GC80~120H~J

Grinding stainless steel: monocrystalline alumina SA46~60G~H

Grinding high-speed steel: white alumina WA60~80J~K

Wheel hardness selection: use a hard wheel for soft workpieces and a soft wheel for hard workpieces.

Common Chemical Heat Treatment Methods

Carburizing: 900~950℃, depth 0.3~2.0mm, for low-carbon steel

Nitriding: 500~540℃, depth 0.1~0.6mm, for steels containing Al/Cr

Carbonitriding: 820~880℃, depth 0.1~0.8mm

Boronizing: 950~1000℃, depth 0.05~0.15mm

Sulphurizing: low temperature, improves wear resistance

Related quick references: Tolerances & FitsSurface RoughnessMaterial Heat TreatmentCast Part DesignGeometrical TolerancesDimension ChainsWelded StructuresSheet Metal StructuresShafting DesignSeal DesignMaterial SelectionHeat TreatmentDatum ReferencingTolerance Principles