MOULDLKnowledge Base3D Model DownloadsMembership
中文版Model Store »
Knowledge Base › Machining Processes › Machining Fundamentals
HomeModels
Table of contents

On this page

Knowledge Base Home

📐 Standard Data

🧮 Calculators

📖 Selection Guides

🏭 Material Grades

❓ Engineer FAQ

🗂 Quick-Reference Categories

❌ Error Case Studies

📚 Technical Articles

Machining Processes · Machining Fundamentals (Quick Reference)

The Three Cutting Elements and Their Selection

【The Three Cutting Elements】

1. Cutting speed vc (m/min) — the velocity of the primary motion

vc = π·D·n/1000

D — tool/workpiece diameter (mm)

n — spindle speed (r/min)

2. Feed f (mm/r) — the feed per revolution

or feed rate vf = f·n (mm/min)

3. Depth of cut ap (mm) — the cutting depth

the perpendicular distance between the machined and the unmachined surfaces

【Selection Principles】

Roughing: large ap first → large f → small vc

ap=2~10mm, f=0.3~1.5mm/r, vc relatively low

Finishing: small ap → small f → high vc

ap=0.1~1mm, f=0.05~0.3mm/r, vc relatively high

【Material Removal Rate Q】

Q = vc·ap·f/1000 (cm³/min)

The larger Q is the higher the efficiency, but it is limited by tool life and machine rigidity

【High Speed Machining (HSM)】

vc reaches 5~10 times the conventional value

Steel: 500~2000m/min

Aluminium: 1000~5000m/min

Features: low cutting force, small heat affected zone, good surface quality

Requires: a rigid machine + a balanced tool + a high speed spindle

【Calculation Example】

Turning C45 steel with a carbide tool

vc=120m/min, workpiece D=50mm

n = 1000vc/(πD) = 1000×120/(π×50) = 764r/min

Select the machine speed n=750rpm

Actual vc = π×50×750/1000 = 117.8m/min

f=0.3mm/r, ap=2mm

Q = 117.8×2×0.3/1000 = 0.071cm³/min

Cutting Force Calculation and Empirical Formulas

【Main Cutting Force Fc Empirical Formula】

Fc = CF·ap^xF·f^yF·vc^nF·KF

CF,xF,yF,nF — coefficients and exponents (from tables, related to the workpiece material and the tool)

KF — correction factor

【Simplified Estimate (Steel)】

Fc ≈ 2000·ap·f (N)

ap, f in mm

Suitable for carbon steel, carbide tools, normal cutting

【Typical Values for C45 Steel】

ap=2mm, f=0.3mm/r, vc=100m/min

Fc ≈ 2000×2×0.3 = 1200N

【Cutting Power】

Pc = Fc·vc/(60×1000) (kW)

Motor power Pmotor = Pc/η

η — machine transmission efficiency (0.7~0.85)

Example: Fc=1200N, vc=100m/min

Pc = 1200×100/60000 = 2kW

Pmotor = 2/0.8 = 2.5kW

【The Three Cutting Force Components】

Fc — main cutting force (tangential, the largest, determines the torque and the power)

Fp — feed force / radial force (causes workpiece deformation)

Ff — feed force (axial)

Typical ratio Fc:Fp:Ff = 1:0.4:0.3

【Factors Influencing the Cutting Force】

1. The higher the workpiece material strength → the higher Fc

For every 100MPa increase in σb, Fc increases by about 15%

2. The higher ap and f → the higher Fc

ap has a greater influence than f (the ap exponent is 0.9~1.0, the f exponent is 0.6~0.8)

3. The larger the rake angle → the lower Fc (less chip deformation)

4. The higher the cutting speed → slightly lower Fc (temperature rises, friction falls)

5. Cutting fluid → Fc drops by 5~15%

6. Tool wear → Fc increases by 20~50%

Cutting Heat and Cutting Temperature

【Sources of Cutting Heat】

1. Shear deformation work in the shear zone (main source, 60~80%)

2. Tool-chip friction work (10~20%)

3. Tool-workpiece friction work (<10%)

【Where the Heat Goes】

Carried away by the chips: 50~80%

Workpiece: 10~30%

Tool: 5~10%

Ambient: <5%

【Cutting Temperature θ Distribution】

The highest temperature is in the middle of the tool-chip contact zone

The rake face temperature is higher than the flank temperature

【Empirical Formula】

θ = Cθ·vc^(0.3~0.5)·f^(0.1~0.2)·ap^(0~0.1)

vc has the greatest influence on the temperature (ap has almost no influence)

【Typical Cutting Temperatures】

Carbon steel with a high speed steel tool: θ<600℃ (the tool limit)

Carbon steel with carbide: θ=600~900℃

Carbon steel with ceramic: θ=800~1200℃

Carbon steel with CBN: θ=1000~1400℃

【Cooling Effect of the Cutting Fluid】

Water based cutting fluid: strong cooling (good heat conductivity)

Oil based cutting fluid: weak cooling but good lubrication

High pressure through-tool coolant: the best cooling effect

【Harm of Excessive Temperature】

1. Accelerated tool wear (diffusion / oxidation)

2. Thermal expansion of the workpiece affects accuracy

3. Surface burns / annealing

4. Increased residual stress

【Measures to Reduce the Temperature】

1. Raise vc appropriately (the temperature rises but there is an optimum range)

2. Reduce f (little influence)

3. Cool adequately (high pressure through-tool coolant)

4. Choose a heat resistant tool material

5. Reduce the tool-workpiece contact length

6. Optimize the rake angle (less chip deformation)

Tool Wear Forms and Tool Life

【Wear Forms】

1. Flank wear VB

The most common, friction between the flank and the workpiece

Wear land width VB

2. Rake face wear (crater wear)

The chip abrades the rake face in the high temperature zone

A crater forms and weakens the cutting edge

3. Boundary wear

Groove wear at the depth of cut

Caused by the work hardened layer of the workpiece

4. Plastic deformation

The cutting edge collapses at high temperature

5. Flaking / chipping

Mechanical impact or thermal shock

6. Diffusion wear

Mutual diffusion of the elements at high temperature (mainly in CBN / ceramic tools)

【Tool Blunting Criterion VB】

Finish turning: VB=0.1~0.3mm

Rough turning: VB=0.4~0.8mm

Finish milling: VB=0.2~0.4mm

【Tool Life T】

T = CT/vc^(1/m)·f^(1/n)·ap^(1/p)

Simplified (fixed ap, f):

vc·T^m = C (Taylor equation)

m — the life exponent (0.1~0.15 for high speed steel, 0.2~0.3 for carbide, 0.4~0.6 for ceramic)

【Typical Tool Lives】

High speed steel turning tool: T=30~60min

Carbide turning tool: T=30~90min

Ceramic tool: T=15~30min (a much higher cutting speed is possible)

【Calculation Example】

Carbide tool turning C45 steel

vc1=120m/min, T1=60min

vc2=150m/min, T2=?

m=0.25

T2 = T1·(vc1/vc2)^(1/m) = 60×(120/150)^4 = 60×0.41 = 24.6min

→ A 25% speed increase gives a 60% life reduction

【Economic Life】

The tool life that corresponds to the lowest machining cost

Teco = (tc·Ct/Cm + 1)·(1/m-1)·tc

tc — tool change time

Ct — tool cost

Cm — machine minute cost

【Measures to Improve Tool Life】

1. Lower vc appropriately (the most significant influence)

2. Optimize the tool geometry angles

3. Use a wear resistant coating (TiN/TiAlN)

4. Cool and lubricate adequately

5. Reduce impact (continuous cutting)

6. Choose a tool material that suits the workpiece

Built-Up Edge Formation and Control, and the Scaling It Causes

【Built-Up Edge (BUE)】

When cutting ductile material at medium speed, the metal at the base of the chip cold welds under the high pressure and friction of the tool-chip contact and builds up at the cutting edge of the rake face

【Formation Conditions】

Temperature: the chip base reaches near the recrystallisation temperature of the material

Carbon steel: vc=20~60m/min (medium speed)

At low speed (<5m/min) the temperature is too low for cold welding

At high speed (>80m/min) the temperature is high enough to soften it so it does not build up

Pressure: high contact pressure between the tool and the chip

Material: ductile materials (low carbon steel / aluminium alloy / stainless steel)

【Effects of the Built-Up Edge】

Advantages: it cuts instead of the edge and protects the tool

Disadvantages:

① It increases the actual rake angle and affects chip flow

② When it detaches, fragments embed in the workpiece surface (scaling)

③ Dimensional instability (the edge height fluctuates)

④ Poor surface roughness

⑤ Work hardening

【Measures to Control the Built-Up Edge】

1. Raise vc into the high speed range (>80m/min) to avoid the medium speed range

2. Lower vc to a very low value (<5m/min) for finishing

3. Increase the rake angle (reduce the contact pressure)

4. Reduce the feed

5. Use cutting fluid (lower the temperature + lubricate)

6. Quench and temper the workpiece (hardness↑, ductility↓)

7. Use coated tools (reduce friction)

【Scaling】

Fish-scale protrusions formed on the workpiece surface by the periodic embedding of built-up edge fragments

Characteristics:

① Distributed along the cutting direction

② Height 5~30μm

③ Greatly reduces the surface quality

④ Hard to remove completely by subsequent polishing

Control: the same measures as for the built-up edge

【Finishing Recommendations】

① Carbide tool high speed finish turning (vc>150m/min)

② High speed steel low speed finish turning (vc<5m/min)

③ Use cutting fluid adequately

④ Quench and temper the workpiece to raise the hardness

Selection and Use of Cutting Fluids

【Functions of the Cutting Fluid】

1. Cooling — carries away the cutting heat

2. Lubrication — reduces friction

3. Cleaning — washes away the chips

4. Rust prevention — protects the workpiece and the machine

【Classification of Cutting Fluids】

1. Water based

a. Emulsion (oil + water + emulsifier)

Concentration 3~10%, good cooling but weak lubrication

Suitable for roughing / steel parts

b. Synthetic cutting fluid (fully synthetic, no mineral oil)

Excellent cooling, weak lubrication

Suitable for grinding / high speed machining

c. Semi-synthetic (micro-emulsion, contains a little oil)

Balances cooling and lubrication

The most versatile

2. Oil based

a. Pure cutting oil (mineral oil / vegetable oil)

Good lubrication, weak cooling

Suitable for finishing / threading / gear cutting

b. Extreme pressure cutting oil (contains S/Cl/P additives)

Reacts with the metal at high temperature to form a lubricating film

Suitable for difficult to machine materials (stainless steel / titanium alloys)

【Cutting Fluid Selection Principles】

Roughing with a heavy load: water based (cooling dominant)

Finishing: oil based or extreme pressure oil (lubrication dominant)

High speed machining: water based or MQL (minimum quantity lubrication)

Grinding: water based synthetic fluid

Aluminium: a dedicated emulsion (prevents corrosion and discoloration)

Cast iron: dry cutting or kerosene (cast iron lubricates itself)

Stainless steel / high temperature alloys: extreme pressure cutting oil

【Methods of Application】

1. Flooding — high flow rate, the most common

2. High pressure through-tool coolant — 50~150bar, the fluid reaches the cutting edge, suited to deep holes / difficult materials

3. Mist cooling — atomised droplets, suited to high speed

4. MQL (minimum quantity lubrication) — 10~100ml/h of oil mist, environmentally friendly

5. Liquid nitrogen cooling — cryogenic, suited to titanium / high temperature alloys

【Cutting Fluid Maintenance】

1. Check the concentration daily with a refractometer

2. Maintain the pH at 8.5~9.5 (rust prevention and odour control)

3. Filter out the chips and sludge

4. Prevent fungal and bacterial growth (biocide)

5. Replace regularly (3~6 months)

【Environmental Protection and Safety】

1. Dispose of the old fluid as hazardous waste

2. Avoid skin contact (allergy)

3. Extract the oil mist (respiratory system)

4. Promote MQL / dry cutting to reduce waste fluid

Work Hardening and Residual Stress

【Work Hardening (Cold Working)】

During cutting, the surface layer of the metal undergoes severe plastic deformation

The dislocation density increases, so the strength and the hardness rise while the ductility and the toughness fall

【Degree of Hardening N】

N = (H-H0)/H0 × 100%

H — surface hardness after machining

H0 — hardness of the workpiece base material

Typical degrees of hardening:

Low carbon steel (S20): N=40~60%

Medium carbon steel (C45): N=30~50%

Stainless steel (304): N=50~80% (hardens easily)

Aluminium alloy: N=10~30%

Hardened layer depth:

General cutting 0.05~0.5mm

Grinding 0.01~0.1mm

Shot peening 0.2~0.8mm

【Factors Influencing Work Hardening】

Factors that increase hardening:

1. A dull tool (heavy wear)

2. A larger feed

3. A large nose radius (strong rubbing)

4. A small rake angle

5. A low cutting speed

6. A workpiece material with high ductility

Measures to reduce hardening:

1. A sharp tool

2. High speed cutting

3. Adequate cooling

4. A reduced feed

【Favourable Effects】

Surface hardness↑ → fatigue strength↑

Surface compressive stress → fatigue strength↑

(Shot peening and roller burnishing deliberately create a hardened layer)

【Unfavourable Effects】

1. Subsequent machining is difficult (the tool wears fast)

2. Surface micro cracks (over-hardening)

3. Reduced corrosion resistance

4. Dimensional instability (deformation from the release of residual stress)

【Residual Stress】

Residual stress exists on the surface after machining

Sources:

1. Uneven plastic deformation (mechanical stress)

2. Thermal deformation (cutting heat)

3. Phase transformation (high temperature grinding)

Tensile stress (+): unfavourable for fatigue

Compressive stress (-): favourable for fatigue

Typical stress distribution:

Surface: tensile or compressive (depending on the process)

Subsurface: the opposite

Depth 0.05~0.5mm

【Residual Stress for Different Processes】

Turning: tensile or compressive on the surface (depending on the conditions)

Grinding: usually tensile on the surface (caused by the high temperature)

Milling: tensile on the surface

Shot peening: compressive on the surface (favourable)

Roller burnishing: compressive on the surface (favourable)

【Measures to Control Residual Stress】

1. Optimize the cutting parameters (reduce the heat input)

2. Use a sharp tool

3. Cool adequately

4. Low temperature ageing after finishing

5. Shot peen strengthening on critical parts

Chip Types and Chip Control

【Types of Chips】

1. Ribbon chip (continuous chip)

A continuous long strip with a smooth underside

Forms when: high speed cutting of ductile material with a large rake angle

Effect: it wraps easily, chip breaking is needed

Surface quality: good

2. Segmental chip (squeezed chip)

The underside is smooth, the top surface is serrated

Forms when: medium speed cutting of ductile material with a small rake angle

Effect: the cutting force fluctuates

Surface quality: medium

3. Elementary chip

Short segments that break off

Forms when: low speed with a small rake angle

Effect: vibration

Surface quality: poor

4. Fragmented chip

Irregular fragments

Forms when: brittle materials (cast iron / brass)

Effect: splashing, impact on the tool

Surface quality: fairly poor

【Chip Control (Chip Breaking)】

Purpose: break the chips up so they can be evacuated

Methods:

1. Chip breaker groove (on the rake face)

Types: straight arc / straight / curved

Width Wn=(3~5)f

Depth Hn=(0.4~0.7)Wn

2. The chip breaker on an indexable insert

Press formed

Designed for the material / the feed

3. Changing the cutting parameters

Increasing the feed f → easier chip breaking

Reducing the cutting speed → easier to break at medium speed

4. Changing the tool angles

Increasing the principal cutting edge angle κr → a thicker chip that breaks easily

5. The workpiece material

Adding S/Pb (free machining steel) makes it break easily

6. The cutting fluid

An oil based cutting fluid → the chips become brittle and break easily

【Evaluation of the Chip Breaking Effect】

Type C: ideal (it breaks after a slight impact)

Type 6~9: fairly good (a short spiral)

Continuous spiral: poor (it wraps around)

Fragmented: too fragmented (high energy consumption, splashing)

Long tight curl: ideal for finishing

【Materials That Are Difficult to Break】

1. Low carbon steel (highly ductile)

2. Stainless steel (work hardening)

3. Pure copper / pure aluminium

4. Titanium alloys

Countermeasures:

① A large feed (a thick chip)

② A large principal cutting edge angle

③ A suitable chip breaker groove

④ An oil based cutting fluid

⑤ Free machining steel (adding S/Pb)

Cutting Temperature Distribution and Tool Thermal Stress

【Cutting Temperature Distribution】

The highest temperature is in the middle of the tool-chip contact zone

About 1/2 of the contact length from the cutting edge

The rake face temperature is higher than the flank temperature

The first deformation zone (the shear plane) is at a moderate temperature

The second deformation zone (the tool-chip contact) is the highest

【Typical Temperature Fields (C45 Steel)】

Tool-chip contact zone: 800~900℃ (carbide)

Near the nose: 600~800℃

The rear of the tool body: 200~400℃

The chips: 500~700℃

The workpiece surface: 100~300℃

【Factors Influencing the Temperature】

1. The cutting speed (the greatest influence)

θ ∝ vc^(0.3~0.5)

Every time vc doubles, the temperature rises by about 40%

2. The feed (a moderate influence)

θ ∝ f^(0.1~0.2)

3. The depth of cut (a small influence)

θ ∝ ap^(0~0.1)

4. The rake angle

A larger rake angle lowers the temperature (less deformation)

But too large raises it again (poor heat dissipation)

5. The workpiece material

σb↑, the thermal conductivity↓ → the temperature↑

Stainless steel / titanium alloys reach high temperatures

6. The cutting fluid

Lowers the temperature by 10~30%

【Tool Thermal Stress】

The tool surface temperature is high and the interior is low

This produces thermal stress (compression at the surface, tension inside)

With intermittent cutting (milling):

At the moment of entry the temperature rises suddenly → compression at the surface

At the moment of exit the temperature drops suddenly → tension at the surface

Cyclic thermal stress → thermal fatigue cracks (a network pattern)

【Thermal Cracking Phenomena】

Carbide / ceramic tools:

A network of cracks appears on the cutting edge

The crack growth causes the insert to break up

Factors influencing it:

1. A large temperature difference

2. Frequent entry and exit (milling)

3. The cutting fluid (sudden cooling makes it worse)

4. The tool material (ceramic is sensitive)

【Preventing Thermal Cracking】

1. Do not use cutting fluid (dry cut the ceramic)

2. Reduce the temperature difference (lower the speed)

3. Choose a heat resistant material (CBN)

4. Optimise the tool geometry (reduce the contact)

5. Use a thermal barrier coating

【Effect of the Cutting Heat on the Workpiece】

1. Thermal expansion (a dimensional change)

Steel: α=12×10⁻⁶/℃

A 50℃ rise: 100mm extends by 0.06mm

2. Thermal deformation (warping)

Thin walled parts / asymmetric parts

3. Surface burning

High grinding temperatures (>500℃) → annealing / cracks

4. Residual stress

Uneven thermo-plastic deformation

【Controlling the Workpiece Temperature Rise】

1. Cool adequately

2. Reduce the cutting data

3. Split it into several passes (heat dissipation)

4. Immerse the workpiece in a cooling liquid

5. Control the ambient temperature

6. Measure at a stable temperature

7. Thermal compensation (CNC)

Economic Accuracy of Machining Methods and Surface Roughness

【Definition of Economic Accuracy】

Under normal production conditions (equipment / process / operator)

The accuracy that a given machining method can achieve

The accuracy at the lowest cost

【Economic Accuracy of the Various Machining Methods】

Turning:

Rough turning IT11~13, Ra12.5~50

Semi-finish turning IT9~10, Ra3.2~6.3

Finish turning IT7~8, Ra0.8~1.6

Precision turning IT6~7, Ra0.4~0.8

Diamond turning IT5, Ra0.1

Milling:

Rough milling IT11~13, Ra12.5~50

Semi-finish milling IT9~11, Ra3.2~12.5

Finish milling IT8~9, Ra1.6~3.2

Precision milling IT7~8, Ra0.8~1.6

Planing:

Rough planing IT11~13, Ra12.5~50

Finish planing IT8~10, Ra1.6~6.3

Drilling:

Drilling IT11~13, Ra12.5~50

Reaming out IT10~11, Ra3.2~12.5

Reaming IT7~9, Ra0.8~3.2

Boring:

Rough boring IT11~13, Ra12.5~50

Semi-finish boring IT9~11, Ra3.2~6.3

Finish boring IT7~8, Ra0.8~1.6

Precision boring IT6, Ra0.4

Grinding:

Rough grinding IT8~9, Ra0.8~1.6

Finish grinding IT6~7, Ra0.4~0.8

Precision grinding IT5~6, Ra0.1~0.4

Super finish grinding IT5, Ra0.025~0.1

Mirror grinding IT5, Ra<0.025

Broaching:

IT7~8, Ra0.4~1.6

Honing:

IT6~7, Ra0.1~0.8

Lapping:

IT5~6, Ra0.012~0.1

Polishing:

Ra0.012~0.8

【Principles for Selecting a Machining Method】

1. Accuracy matching

Select the method according to the required IT grade and Ra

Example: IT7/Ra0.8 → finish turning / finish grinding / reaming

2. The surface shape

External diameter: turning / grinding

Internal bore: drilling / boring / grinding / reaming / broaching

Flat surface: milling / planing / grinding / broaching

Thread: turning / milling / grinding / rolling

Tooth form: milling / hobbing / shaping / grinding

3. The workpiece material

Steel: turning / milling / grinding

Cast iron: turning / milling / grinding (it is not suitable for reaming)

Hardened steel: grinding / turning (hard turning)

Aluminium: turning / milling / diamond turning

Stainless steel: turning (a sharp tool) / grinding

4. The batch size

Single pieces: turning / milling / drilling (general purpose)

Small batches: CNC turning / milling

Large batches: special purpose machines / broaching / transfer machines

Mass production: automated lines / NC flow lines

5. Cost

The higher the accuracy the higher the cost index

Ra0.8 vs Ra0.1 costs 10 times more

【Relationship Between Accuracy and Cost】

Raising the accuracy by one grade raises the cost by about 50~100%

Lowering Ra by one grade raises the cost by about 30~50%

【Example of an Allowance Distribution】

Requirement: IT6/Ra0.4 on an external diameter φ30:

1. Rough turning (leave 2mm) IT11

2. Semi-finish turning (leave 0.5mm) IT9

3. Finish turning (leave 0.2mm) IT7

4. Rough grinding (leave 0.05mm) IT7

5. Finish grinding IT6/Ra0.4

【Avoiding Over-Machining】

Unnecessary accuracy / roughness increases the cost

Example: a non mating surface at Ra6.3 does not need Ra0.8

a general joint at IT8 does not need IT6

Machine Tool Model Coding and Machine Tool Selection

【Machine Tool Model Coding (GB/T 15375)】

Example: CA6140

C — the category (a lathe)

A — the structural characteristic (improved)

6 — the group (a floor standing / ordinary lathe)

1 — the series (an ordinary lathe)

40 — the main parameter (the maximum swing of 400mm)

The main machine tool categories:

C — lathes

Z — drilling machines

T — boring machines

M — grinding machines

X — milling machines

B — planing / slotting machines

L — broaching machines

Y — gear cutting machines

S — thread cutting machines

G — cut-off machines

Q — others

【Common Machine Tools】

1. Lathes

CA6140 ordinary lathe (swing 400)

CK6140 CNC lathe (swing 400)

C6132 ordinary lathe (swing 320)

CNC turning center (with a power turret)

2. Milling machines

X62W horizontal milling machine

X52K vertical milling machine

XK5032 CNC vertical mill

Machining center VMC850 (vertical)

HMC (horizontal machining center)

3. Drilling machines

Z3040 radial drilling machine (a maximum hole of 40)

Z5150 vertical drilling machine

Z4012 bench drilling machine

4. Boring machines

T68 horizontal boring machine

TX6213 CNC boring machine

Coordinate boring T4240 (precision)

5. Grinding machines

M1432 external cylindrical grinder

M7120 surface grinder

M2110 internal cylindrical grinder

MK2120 CNC internal grinder

【Factors to Consider When Selecting a Machine Tool】

1. Matching the machining capability

The workpiece size < the maximum size of the machine

The workpiece weight < the capacity of the machine

The power > the power required by the cutting

2. Matching the accuracy

The workpiece accuracy requirement < the machine accuracy

Select a precision machine for an IT6 workpiece

Select an ordinary machine for a general workpiece

3. Matching the rigidity

Heavy roughing cuts → a rigid machine

Finishing → a high accuracy machine

Slender shafts → a steady rest / follower rest

4. Matching the batch size

Single pieces and small batches: general purpose machines

Medium batches: CNC machines

Large batches: special purpose machines / automated lines

5. Cost

A high accuracy machine is expensive (select one that is good enough)

Use a large machine for large parts (sensible)

Fully utilise the capability of the machine

【Machine Tool Accuracy Grades】

Standard grade P

Precision grade M

High accuracy grade G

Ultra precision grade C

【Typical Machine Tool Accuracy】

Ordinary lathe:

Roundness 0.01

Cylindricity 0.02/300

Flatness 0.02/300

CNC lathe:

Positioning accuracy 0.01

Repeatability 0.005

Roundness 0.005

Machining center:

Positioning accuracy 0.005~0.01

Repeatability 0.003~0.005

Roundness 0.005

External cylindrical grinder:

Roundness 0.003

Cylindricity 0.005/300

Ra0.4

Coordinate boring machine:

Positioning accuracy 0.003

Hole spacing 0.005

【Machine Tool Maintenance】

1. Daily checks (lubrication / air pressure / oil level)

2. Regular accuracy checks

3. Guideway lubrication (an oil circuit / automatic)

4. Spindle warm-up (precision)

5. Cleaning (prevents rust / prevents chips)

6. A vibration damping foundation

7. A temperature controlled environment (precision)

8. Regular calibration (a laser interferometer)

Machining Technology for Difficult to Machine Materials

【Cutting Stainless Steel】

Characteristics: severe work hardening, poor thermal conductivity, affinity with the tool

Tooling: the YG series (no Ti) / coated / YW

Parameters: vc=50~100m/min (carbide)

f=0.05~0.2mm/r (reduces the hardening)

ap>0.15mm (cuts past the hardened layer)

Precautions:

① A sharp tool (a large rake angle)

② Cool adequately

③ Avoid forming a built-up edge in the medium speed range

④ Climb milling is better than conventional milling

【Cutting Titanium Alloys】

Characteristics: very poor thermal conductivity, chemical activity, a low elastic modulus

Tooling: the YG series / PCD (for finishing)

Parameters: vc=30~60m/min

f=0.05~0.15mm/r

ap=0.5~3mm

Precautions:

① A low speed (prevents a high temperature)

② Cool adequately (titanium has poor thermal conductivity)

③ A sharp tool

④ Good rigidity (large elastic springback)

⑤ Avoid chloride cutting fluids (stress corrosion)

【Cutting Super Alloys】

Characteristics: high hot strength, work hardening, poor thermal conductivity

Tooling: coated carbide / ceramic / CBN

Parameters:

vc=15~50m/min (carbide)

vc=100~300m/min (ceramic)

f=0.05~0.15mm/r

Precautions:

① A low speed with a deep cut

② Cool adequately

③ A sharp tool

④ A rigid system

【Cutting Hardened Steel (Hard Turning)】

Hardness HRC 45~65

Tooling: CBN / ceramic / coated carbide

Parameters:

vc=100~200m/min (CBN)

f=0.05~0.15mm/r

ap=0.1~0.5mm

Advantages: turning instead of grinding

Precautions: a sharp tool, good rigidity, adequate cooling

【Cutting Engineering Plastics】

Characteristics: poor thermal conductivity, elastic springback, a large thermal expansion

Tooling: high speed steel / carbide (sharp)

Parameters: vc=100~300m/min

f=0.05~0.2mm/r

Precautions:

① A large rake angle (sharp)

② Cool adequately (air / water)

③ A sharp tool (prevents melting)

④ Support the thin walled parts (prevents deformation)

Green Machining and Sustainable Manufacturing

【Concept of Green Machining】

Reduce the cutting fluid consumption

Lower the environmental burden

Protect the health of the workers

【Environmental Impact of Cutting Fluids】

1. Waste fluid disposal (hazardous waste)

2. Oil mist (the respiratory system)

3. Skin allergies

4. The cooling energy consumption

5. Chip contamination (with oil)

【Green Machining Methods】

1. Dry machining

No cutting fluid at all

Conditions:

① The tool is heat resistant (ceramic / CBN / coated)

② The workpiece material is suitable (cast iron / aluminium alloy)

③ High speed cutting (the heat is carried away by the chips)

④ The machine removes the chips well

Suitable for:

- Cast iron machining (it lubricates itself)

- High speed aluminium alloy machining

- High speed machining of some steel parts

Limitations:

- Stainless steel / titanium alloys (a high temperature)

- Deep holes / blind holes

- Low speed heavy cuts

2. MQL (Minimum Quantity Lubrication)

A very small amount of oil (10~100ml/h) + compressed air

The oil mist is sprayed into the cutting zone

Advantages:

① An extremely small amount of oil (saves 99%)

② No waste fluid disposal

③ The workpieces and the chips stay clean

④ The health of the workers

Disadvantages:

① Weak cooling capability

② Not suited to heavy loads

③ The equipment investment

④ The oil mist control

Applications:

- Aluminium alloy machining

- Cast iron machining

- Finishing of some steel parts

- Thread cutting / reaming

- Gear machining

3. Cold air cutting

Cold air at -20~-50℃

Replaces the cutting fluid cooling

Advantages:

① No liquid

② A good cooling effect

③ The workpieces stay clean

Disadvantages:

① The equipment is complex (refrigeration)

② A high energy consumption

③ No lubrication

4. Liquid nitrogen cooling

Liquid nitrogen at -196℃ is sprayed

Cryogenic cooling

Advantages:

① An extremely low temperature (titanium / super alloys)

② No pollution

③ Increases the tool life

④ Improves the surface quality

Disadvantages:

① Expensive

② Storage and transport

③ Safety (frostbite)

5. CO2 cooling

CO2 snow is sprayed

A low temperature plus cleaning

Application: titanium / nickel base alloys

【Green Tooling】

1. Coated tools (no cutting fluid)

TiAlN/Al2O3 for thermal insulation

2. Self lubricating tools

Contain a solid lubricant (WSe2 / MoS2)

3. Simulation based design

Optimise the tool geometry (reduces the cutting heat)

【Trends in Green Manufacturing】

1. Legislation restricting cutting fluids (the EU)

2. Rising waste fluid disposal costs

3. Worker health requirements

4. ISO 14000 environmental management

5. Customer green requirements (automotive / electronics)

【Implementing Green Machining】

1. Assess the existing machining (can it be dry cut)

2. Optimise the tools / the parameters

3. Pilot the MQL

4. Roll it out gradually

5. Monitor the quality / the tool life

6. Train the operators

Machining Vibration and Chatter Suppression

【Types of Vibration】

1. Forced vibration

External excitation (the machine / the foundation / an imbalance)

The frequency = the excitation frequency

Eliminating the excitation source is enough

2. Self excited vibration (chatter)

It is sustained by the cutting process itself

The frequency is close to the natural frequency of the system

Regenerative chatter is the most common

3. Regenerative chatter

The waviness left by the previous cut → the chip thickness changes in this cut → the force changes → a new waviness

A self exciting loop

【Characteristics of Chatter】

① A specific frequency (the natural frequency of the machine / the workpiece / the tool)

② It is sensitive to the cutting parameters (the speed / the depth of cut)

③ Clear chatter marks on the surface

④ A harsh noise

⑤ It accelerates the tool wear

【Methods of Chatter Suppression】

1. Change the cutting parameters

- Increase / decrease the cutting speed (avoid the unstable zone)

- Reduce the depth of cut (the main factor)

- Increase the feed (reduce the overlap)

2. Change the tool geometry

- Increase the principal cutting edge angle κr (reduce the radial force)

- Increase the rake angle (reduce the cutting force)

- Reduce the nose radius

- Reduce the clearance angle (increases the damping)

- A variable helix / a variable pitch (milling cutters)

3. Increase the system rigidity

- A short tool overhang

- A large diameter holder

- A damping holder (damping)

- A steady rest / a follower rest (the workpiece)

4. Increase the damping

- A damping bar (filled with tungsten / mercury inside)

- Damping materials (rubber / polymer)

- A vibration damping foundation for the machine

5. The cutting fluid

- Lubricate adequately to reduce the friction

6. Active control

- A piezoelectric actuator adjusts the tool

- Real time vibration monitoring with feedback

【Stability Lobe Diagram (Lobe Diagram)】

The horizontal axis: the cutting speed

The vertical axis: the depth of cut

The stable zone (a large depth of cut is possible) / the unstable zone (it chatters even with a small depth of cut)

Application: choose the cutting parameters in the stable zone

【Typical Chatter Scenarios】

1. Boring (a long boring bar overhang)

2. Turning slender shafts

3. Milling thin walls

4. Drilling deep holes

5. Deep slots with an end mill

【Vibration Measurement】

1. An accelerometer

2. A vibration meter

3. A spectrum analyser

4. A microphone (a simple method)

【Permissible Vibration Values (ISO 10816)】

Small machine tools: <2.8mm/s

Medium machine tools: <3.5mm/s

Large machine tools: <4.5mm/s

Cutting Simulation and Finite Element Analysis

【Purpose of Cutting Simulation】

1. Predict the cutting force / the temperature

2. Optimise the tool geometry

3. Optimise the cutting parameters

4. Predict the tool wear

5. Predict the surface quality

6. Reduce the trial cutting cost

【Simulation Methods】

1. Analytical methods (fast, simplified)

The shear angle model

The empirical cutting force formulas

2. The finite element method (detailed, slow)

Build the workpiece and the tool model

Mesh generation (refined at the tool-chip contact)

The material model (Johnson-Cook)

The friction model

Heat transfer

3. The discrete element / smooth particle method

It handles large deformation and chip fracture

【Commercial Software】

1. AdvantEdge

Specialist cutting simulation

2D/3D

Supports turning / milling / drilling

2. Deform

General forming + cutting

Large deformation

3. ABAQUS/ANSYS

General finite element

Custom modelling

4. Third Wave Systems

The Production Module

Shop floor level optimisation

【Material Model (Johnson-Cook)】

σ = (A + Bεⁿ)(1 + C·ln(ε̇/ε̇0))(1 - T*m)

A — the yield strength

B, n — the strain hardening

C — the strain rate sensitivity

m — the temperature sensitivity

Example (C45 steel):

A=553MPa, B=542MPa, n=0.258

C=0.0134, m=1.05

【Simulation Outputs】

1. The cutting forces (three directions)

2. The cutting temperature (the distribution)

3. The stress / strain distribution

4. The chip shape

5. The tool stress / temperature

6. The residual stress in the machined surface

【Application Scenarios】

1. Difficult to machine materials (titanium / super alloys)

2. Tool optimisation (the rake angle / the edge)

3. Optimising the cutting parameters

4. Evaluating the machinability of new materials

5. Predicting the surface integrity

【Simulation Verification】

1. The cutting force (a dynamometer)

2. The cutting temperature (a thermocouple / infrared)

3. The chip shape (a comparison)

4. The tool wear (a comparison)

5. The residual stress (X-ray)

【Advantages and Disadvantages】

Advantages:

① Reduces the trial cutting cost

② Optimises the parameters

③ Predicts the performance

④ Helps to understand the mechanisms

Disadvantages:

① The model is simplified (the accuracy is limited)

② A long computation time

③ It is difficult to obtain the material parameters

④ It requires an expert

【Application Trends】

1. The digital twin (real time simulation + reality)

2. AI assisted optimisation

3. Cloud based simulation services

4. Integration with CAM

Thermal Compensation Technology in Machining

【Sources of Machine Tool Thermal Deformation】

1. The heat from the spindle motor

2. The cutting heat

3. The friction heat (the leadscrew / the guideways)

4. Changes in the ambient temperature

5. The heat from the hydraulic system

Thermal deformation accounts for 30~50% of the machine tool error

【Typical Thermal Deformations】

1. The thermal expansion of the spindle (in the Z direction)

A 1℃ rise in the spindle temperature → 5~10μm of expansion (over 100mm)

Running at 5000rpm for 1 hour → 0.02~0.05mm of expansion

2. The thermal expansion of the leadscrew (in the X/Y directions)

The expansion of a long leadscrew is more significant

A 1℃ rise in a 1m leadscrew → 12μm of expansion

3. The thermal bending of the column

A temperature difference between the inside and the outside → bending

It affects the accuracy in the Y direction

4. The thermal deformation of the table

It affects the flatness

【Methods of Thermal Compensation】

1. Warm-up (the basis)

Idle the machine for 15~30min after switching it on

Bring the machine to a thermal equilibrium

High accuracy machining requires a warm-up

2. A temperature controlled workshop

20±1~2℃ (precision)

20±5℃ (general)

The humidity 50±10%

3. Oil cooling / water cooling

Spindle oil cooling (20±0.5℃)

A hollow cooled leadscrew

Air conditioning the electrical cabinet

4. A symmetrical structure design

A thermally symmetrical machine structure

Reduces the thermal bending

5. Active thermal compensation (a CNC function)

a. The temperature sensor layout

Multiple points on the spindle / the leadscrew / the environment

b. Building a thermal error model

Multivariate regression / a neural network

c. Real time compensation

The CNC parameters are corrected automatically

The compensation effect: reduces the thermal error by 70~90%

【Spindle Thermal Expansion Compensation】

Measurement: the expansion of the spindle at different temperatures

Model: ΔL = f(T)

Compensation: the Z axis moves back by ΔL automatically

Example:

The spindle temperature rises 20℃

ΔL = 20×8 = 160μm

The Z axis is compensated by -0.16mm

【Leadscrew Thermal Compensation】

Measurement: the expansion of the leadscrew at different temperatures / positions

Model: ΔL(x,T) = α·x·(T-T0)

Compensation: each position is corrected automatically

【Thermal Error Modelling】

1. Multivariate linear regression

E = a0 + a1·T1 + a2·T2 + ...

T1,T2 — the temperature measuring points

2. A neural network

Non linear modelling

High accuracy

Training data is needed

3. The finite element method

The thermal analysis of the machine tool

Optimises the structure

【Temperature Sensor Layout】

1. The spindle bearing outer ring

2. The spindle motor

3. The leadscrew nut

4. The leadscrew bearings

5. The column / the bed

6. The ambient

7. The coolant

Usually 6~16 sensors

【Implementing the Compensation】

1. Measurement (a laser interferometer / a ball bar)

2. Modelling (regression / a neural network)

3. Calibration (the parameters are entered into the CNC)

4. Validation (checked by actual machining)

5. Periodic recalibration

【Effect of the Thermal Compensation】

Before compensation: a thermal error of 0.05~0.1mm

After compensation: a thermal error of 0.01~0.02mm

The accuracy improves by 3~5 times

【Other Ways of Reducing the Thermal Error】

1. Choose a low thermal expansion material

Invar (α≈1×10⁻⁶)

Ceramic (α≈3×10⁻⁶)

Granite (α≈8×10⁻⁶)

2. Active temperature control

Internal water cooling of the spindle

A hollow cooled leadscrew

Heat pipe dissipation

3. Constant temperature cutting fluid

20±0.5℃

Reduces the thermal deformation of the workpiece

Tool Monitoring Technology in Machining

【Purpose of Tool Monitoring】

1. Prevent tool breakage (it damages the workpiece / the machine)

2. Change the tool in time (guarantees the quality)

3. Optimise the tool life

4. Reduce the downtime

5. It is essential for automation

【Tool Condition States】

1. A new tool (sharp)

2. The initial wear (rapid)

3. Normal wear (slow)

4. Rapid wear (rapid, the tool should be changed)

5. Breakage (chipping / fracture)

【Monitoring Methods】

1. Direct measurement

a. Machine vision

A camera photographs the tool

Image processing identifies the wear

High accuracy

It requires the machine to be stopped

b. A contact probe

Measures the tool tip position / shape

On-machine measurement

c. Laser measurement

A laser measures the tool contour

Non contact

2. Indirect measurement (on-line)

a. Cutting force monitoring

A dynamometer / a force measuring bearing

An increase in the force → the wear

A sudden change in the force → the breakage

b. Power / torque monitoring

The spindle motor power

Simple, universal

Low sensitivity

c. Vibration monitoring

An accelerometer

A change in the vibration spectrum

Suited to milling

d. Acoustic Emission (AE)

An acoustic emission sensor

It detects high frequency elastic waves

Very sensitive

A strong signal at the moment of breakage

e. Temperature monitoring

A thermocouple / infrared

The wear → the temperature rises

f. Surface roughness

On-line optical measurement

The wear → Ra rises

g. Chip shape

A camera identifies the chips

A change reflects the tool condition

【Acoustic Emission Monitoring (AE)】

Principle:

Material deformation / fracture releases elastic waves

The frequency is 100kHz~1MHz

Signal characteristics:

Normal cutting: a continuous low amplitude AE

Tool wear: the AE amplitude increases

Tool breakage: a sudden high amplitude AE

Advantages:

① Very high sensitivity

② A fast response (ms level)

③ Suited to detecting breakage

Disadvantages:

① The signal is complex

② It is easily disturbed

③ It needs an empirical threshold

【Cutting Force Monitoring】

Measurement:

1. A dynamometer (under the table)

High accuracy but expensive

Suited to the laboratory

2. A force measuring bearing

The sensor is integrated in the bearing

It measures the force indirectly

Suited to production

3. The spindle power

The motor current → the torque → the force

Simple, universal

Low accuracy

The pattern of the force change:

Normal wear: the force gradually increases by 10~30%

Rapid wear: the force jumps

Breakage: a sudden force change + vibration

【Tool Life Management (a CNC Function)】

1. The tool usage time statistics

The accumulated usage time of each tool

Set the life threshold

It reminds you to change the tool when the time is reached

2. Tool wear compensation

The tool length / radius compensation

It is adjusted according to the wear amount

3. Tool breakage detection

A conductivity check (contact type)

Measure the tool tip position

An anomaly → stop the machine

【Intelligent Tool Management】

1. RFID tool identification

An RFID tag on the tool

It records: the specification / the life / the usage history

2. A tool database

The state of each tool

The historical data

3. AI prediction

It predicts the life from the historical data

It optimises the tool change time

4. Cloud management

Several machines share the tool data

The supplier provides remote support

【Application Scenarios】

1. Unattended production (FMS)

2. Critical operations (aerospace / medical)

3. High value tools (CBN/PCD)

4. Difficult to machine materials

5. Automatic tool change systems

【Implementation Considerations】

1. The cost versus the benefit

2. The system reliability

3. The false alarms / the missed detections

4. The integration with the CNC

5. The operator training

Related quick references: Cutting Tool MaterialsTool GeometryTurning ProcessMilling ProcessDrilling ProcessBoring ProcessGrinding ProcessMachining AllowanceProcess SequencingTypical ProcessesCNC ProgrammingFixture DesignSpecial Machining Processes

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL