MOULDLKnowledge Base3D Model DownloadsMembership
中文版Model Store »
Knowledge Base › Machining Processes › Special Machining Processes
HomeModels
Table of contents

On this page

Knowledge Base Home

📐 Standard Data

🧮 Calculators

📖 Selection Guides

🏭 Material Grades

❓ Engineer FAQ

🗂 Quick-Reference Categories

❌ Error Case Studies

📚 Technical Articles

Machining Processes · Special Machining Processes (Quick Reference)

EDM Principle and Applications

【Principle of EDM】

Pulse discharge between the workpiece and the tool electrode

The discharge channel reaches a very high temperature (8000~12000℃) that melts / vaporises the metal

The dielectric fluid flushes away the melted metal

Characteristics:

① No contact (no cutting force)

② Any conductive material can be machined (regardless of hardness)

③ Complex shapes can be machined

④ High accuracy (±0.005~0.02)

⑤ Slow (a low material removal rate)

⑥ The tool electrode wears

【Types】

1. Sinker EDM

The electrode shape is copied to the workpiece

Suited to cavities / die holes

Electrode: graphite / pure copper

2. Wire EDM (WEDM)

A thin metal wire (0.1~0.3mm) acts as the electrode

Cuts a complex profile

Suited to templates / punches and dies / narrow slots

3. EDM grinding

A rotating electrode grinds

4. EDM surface hardening

The tool electrode material is deposited onto the workpiece

【Machining Parameters】

Pulse width: 1~2000μs (larger for roughing)

Pulse interval: 10~500μs

Peak current: 1~200A

Open circuit voltage: 80~300V

Polarity: the workpiece positive / negative (depending on the case)

Roughing: a large pulse width / large current, high efficiency, Ra5~10

Finishing: a small pulse width / small current, low efficiency, Ra0.8~1.6

【Electrode Wear】

Graphite electrode: low wear (0.1~1%)

Pure copper electrode: moderate wear (1~5%)

Methods of reducing the wear:

① Select a suitable electrode material

② Optimise the electrical parameters (pulse width / polarity)

③ Use multiple electrodes (separating roughing and finishing)

【WEDM Parameters】

Molybdenum wire diameter: 0.1~0.25mm

Copper wire diameter: 0.1~0.3mm (fast wire)

Wire speed: 8~11m/s (fast wire) / 100~200m/min (slow wire)

Cutting speed:

Fast wire: 20~80mm²/min

Slow wire: 50~200mm²/min

Accuracy:

Fast wire: ±0.01~0.02mm, Ra1.6~3.2

Slow wire: ±0.003~0.008mm, Ra0.4~1.6

【Applications】

1. Mould cavities (injection / die casting / forging moulds)

2. Narrow slots / small holes (deep holes down to 0.1mm)

3. Carbide machining

4. Machining after quenching (avoids cracking)

5. Irregular holes of complex shapes

6. Aerospace super alloys

【EDM vs Mechanical Machining】

Advantages of EDM:

① Not limited by the material hardness

② Complex shapes are formed in one setup

③ No cutting force deformation

④ Can be machined after quenching

Disadvantages of EDM:

① Slow

② A surface altered layer (0.01~0.1mm)

③ High equipment cost

④ The tool electrode has to be made

【Surface Altered Layer】

The EDM surface has a recast layer + a heat affected layer

Recast layer: hard and brittle, prone to cracking

Heat affected layer: quenched and tempered structure

Measures to eliminate it:

① Remove it in the finishing operation

② Subsequent polishing

③ Chemical dissolution removal

Electrochemical Machining and Electroforming

【Principle of Electrochemical Machining (ECM)】

The workpiece (anode) and the tool (cathode) are in an electrolyte

After the current is applied the anode dissolves

The tool feeds in, forming the shape of the workpiece

Characteristics:

① No contact, no cutting force

② Not limited by the material hardness

③ The tool does not wear

④ Good surface quality (no altered layer)

⑤ A higher efficiency than EDM

⑥ The equipment is complex and the cost is high

【Electrolyte】

Common: NaCl / NaNO3 / NaClO3 aqueous solutions

Concentration: 10~25%

Pressure: 0.5~2MPa (flushes away the electrolysis products)

Temperature: 30~50℃

【Machining Parameters】

Voltage: 8~24V (DC)

Current density: 10~200A/cm²

Gap: 0.05~0.8mm

Feed speed: 0.1~1mm/min

【Material Removal Rate】

V = η·I·ω/(ρ·A·nF)

Simplified: V removal ∝ I

A large current means a fast removal

【Applications】

1. Turbine blade profiles

2. Gun barrel rifling

3. Integral gears (electroformed gears)

4. Deep holes / irregular holes

5. Chamfering / deburring

6. Difficult to machine materials (super alloys / titanium)

【Accuracy】

Dimensional accuracy: ±0.05~0.2mm

Surface Ra: 0.4~3.2

Fillet radius: 0.2~0.5mm

【Electroforming】

Uses the principle of electrodeposition

The master mould (conductive) acts as the cathode

The metal is electrodeposited onto the master mould

The product is released from the mould

Characteristics:

① Extremely high copying accuracy (nanometer level)

② Extremely complex shapes can be produced

③ Suited to thin walled parts

④ A long cycle (the deposition is slow)

【Electroforming Materials】

Nickel: the most common (good strength and toughness)

Copper: conductive parts

Iron: structural parts

Gold / silver: decorative / precision

Alloys: nickel cobalt / nickel iron

【Electroforming Process】

1. Make the master mould (metal / non metal with a conductive layer)

2. Surface treatment (a release agent)

3. Electrodeposition (several hours to several days)

4. Machine the back face

5. Release from the mould

6. Finishing

【Electroforming Applications】

1. Mould cavities (precision injection moulds)

2. Waveguides (aerospace electronics)

3. Nozzles (diesel injector nozzles)

4. Engraving plates / printing plates

5. Mirrors (telescopes)

6. Micro parts (MEMS)

【Accuracy】

Copying accuracy: <0.1μm

Surface roughness: the same as the master mould

Minimum wall thickness: 0.01mm

Maximum thickness: 5mm (a time limit)

Laser Processing Technology

【Principle of Laser Processing】

A high energy density laser beam (10⁴~10⁹W/cm²)

Focused onto the workpiece surface

Instantly melts / vaporises the metal

Characteristics:

① No contact (no tool wear)

② High accuracy

③ A small heat affected zone

④ Any material can be machined

⑤ Easy to automate

【Types of Laser】

1. CO2 laser (10.6μm infrared)

Power: 100~10000W

Suitable for: non metals / steel / aluminium cutting

2. Fibre laser (1.07μm)

Power: 50~30000W

Suitable for: metal cutting / welding / cladding

High efficiency, low maintenance

3. YAG laser (1.06μm)

Power: 50~500W (pulsed)

Suitable for: precision drilling / marking

4. Excimer laser (UV)

A short wavelength, cold processing

Suitable for: precision micro machining / medical

5. Picosecond / femtosecond laser (ultra short pulse)

Cold processing (no heat affected zone)

Suitable for: micro and nano machining

【Laser Cutting】

Materials: steel / aluminium / copper / stainless steel / plastics / wood

Thickness:

Carbon steel: 0.5~25mm

Stainless steel: 0.5~15mm

Aluminium: 0.5~10mm

Accuracy: ±0.1~0.3mm

Kerf: 0.1~0.5mm

Surface Ra: 3.2~12.5

Cutting speed (1500W fibre):

1mm steel: 10~20m/min

3mm steel: 3~6m/min

6mm steel: 1~2m/min

Assist gas:

Oxygen (carbon steel): supports combustion, increases the speed

Nitrogen (stainless steel / aluminium): prevents oxidation

Air (thin sheet): economical

【Laser Welding】

Characteristics:

① Deep penetration welding (the keyhole effect)

② A large weld depth to width ratio (10:1)

③ A small heat affected zone

④ Little distortion

⑤ Fast

Parameters:

Power: 1000~10000W

Speed: 1~10m/min

Focus: ±0.5mm

Applications:

Automotive bodies (galvanised sheet)

Batteries (lithium battery packaging)

Stainless steel sheet

Titanium alloy aerospace parts

【Laser Drilling】

Hole diameter: 0.01~1mm

Depth to diameter ratio: 10~20

Accuracy: ±0.005mm

Applications:

Fuel injector nozzles (0.1~0.3mm)

Turbine blade cooling holes

Diamond wire drawing dies

Micro holes in printed circuit boards

【Laser Cladding】

The laser melts the metal powder onto the substrate

Forming a metallurgically bonded coating

Characteristics:

① High bonding strength (metallurgical bond)

② A small heat affected zone (the substrate does not deform)

③ Worn parts can be repaired

④ The composition can be customised

Applications:

Engine block repair

Mould repair

Journal repair

Wear resistant and corrosion resistant coatings

【Laser Surface Treatment】

1. Laser hardening (transformation hardening)

HRC rises by 5~15

Extremely small deformation

2. Laser melting (remelting)

Refines the structure

Improves the corrosion resistance

3. Laser shock peening

Surface compressive stress

Raises the fatigue strength

【Laser Marking】

Laser engraving / QR codes / serial numbers

Permanent identification

Non contact

Suitable for: metal / plastic / ceramic / glass

Waterjet Cutting and Ultrasonic Machining

【Principle of Waterjet Cutting】

A high pressure water jet (200~600MPa) passes through a small orifice (0.1~0.5mm)

The speed can reach 1000m/s (3 times the speed of sound)

The impact cuts the material

Types:

1. Pure water jet cutting

Water only

Suited to soft materials: rubber / plastics / paper / food

2. Abrasive water jet cutting (AWJ)

Abrasive (garnet) is added to the water

Suited to hard materials: steel / aluminium / titanium / ceramics / glass / stone

Characteristics:

① No heat affected zone (cold cutting)

② A flat cut surface (no burr)

③ Any material can be cut

④ A narrow kerf (0.5~1.5mm)

⑤ Slower than laser cutting

⑥ Accuracy ±0.1~0.3mm

【Abrasive Waterjet Parameters】

Pressure: 300~600MPa

Flow: 2~5L/min

Abrasive: garnet sand 80#~120#

Abrasive flow: 200~500g/min

Cutting speed:

10mm steel: 50~200mm/min

50mm steel: 10~30mm/min

20mm aluminium: 200~500mm/min

20mm glass: 100~300mm/min

【Waterjet Applications】

1. Metal cutting (no heat affected zone)

2. Composite materials (carbon fibre / glass fibre reinforced plastics)

3. Glass / stone / ceramics

4. Food (cakes / meat / frozen goods)

5. Demolition (concrete / steel structures)

【Principle of Ultrasonic Machining】

The tool vibrates at an ultrasonic frequency (20~40kHz)

In an abrasive slurry the tool impacts the abrasive

The abrasive impacts and breaks the workpiece material

Characteristics:

① Suited to hard brittle materials (glass / ceramics / semiconductors)

② No heat affected zone

③ Good surface quality (Ra0.2~0.8)

④ High accuracy (±0.01)

⑤ Slow

【Ultrasonic Parameters】

Frequency: 20~40kHz

Amplitude: 10~50μm

Abrasive: boron carbide / silicon carbide / diamond

Grit size: 100#~600#

Pressure: 0.1~1MPa

【Ultrasonic Applications】

1. Drilling glass / ceramics

2. Semiconductor dicing

3. Gemstone processing

4. Wire drawing die holes

5. Engraving complex shapes

【Ultrasonic Assisted Machining】

Ultrasound is superimposed on conventional machining

1. Ultrasonic vibration turning

The tool vibrates ultrasonically

Reduces the cutting force by 50~80%

Improves the surface quality

Suited to difficult to machine materials

2. Ultrasonic vibration grinding

The wheel or the workpiece vibrates ultrasonically

Improves chip evacuation

Reduces the grinding force

Reduces burning

3. Ultrasonic assisted drilling

The drill vibrates ultrasonically

Improves chip evacuation

Reduces the drill wear

Suited to deep holes / titanium alloys

4. Rotary ultrasonic machining (RUM)

A diamond tool rotates with ultrasonic vibration

Suited to ceramics / glass / composite materials

The efficiency is 10 times higher than pure ultrasonic

【Advantages】

1. Reduces the cutting force

2. Improves the accuracy

3. Extends the tool life

4. Improves the surface quality

5. Suited to difficult to machine materials

【Limitations】

1. The equipment is complex (a ultrasonic generator + a transducer)

2. Special tooling and fixtures

3. The amplitude is limited (<50μm)

4. High cost

3D Printing (Additive Manufacturing) Processes

【Principle of 3D Printing】

The material is built up layer by layer to form a three dimensional solid

It differs from subtractive (machining) processes

【Classification of Processes】

1. SLA stereolithography

An ultraviolet laser cures a liquid photosensitive resin

High accuracy (±0.1mm)

Surface Ra6~12

Material: photosensitive resin (ABS / PP like)

Applications: prototypes / precision parts / jewellery / dental models

2. SLS selective laser sintering

A laser sinters the powder (Nylon / PA12 / metal)

Medium accuracy (±0.2mm)

No support needed (the powder self supports)

Materials: nylon / polystyrene / metal

3. SLM selective laser melting

A laser completely melts the metal powder

Density >99%

The mechanical properties approach those of forgings

Materials: 316L / Ti6Al4V / AlSi10Mg / Inconel718

Applications: aerospace / medical / complex structural parts

4. FDM fused deposition modelling

A hot filament is extruded and deposited

Low accuracy (±0.3mm)

Low cost, suited to desktop use

Materials: ABS / PLA / PETG / nylon

5. 3DP binder jetting

A binder is jet printed onto the powder

Suitable for: sand moulds / ceramics / metal

Fast, low cost

6. LOM laminated object manufacturing

Thin sheets are stacked, cut and bonded

Paper / plastic / metal sheet

Suited to large prototypes

7. DED directed energy deposition

A laser melts the fed powder / wire

Suitable for: repair / large parts / gradient materials

【Metal 3D Printing (SLM) Parameters】

Laser power: 200~1000W

Scan speed: 500~2000mm/s

Layer thickness: 20~100μm

Powder particle size: 15~45μm

Shielding gas: argon / nitrogen

Density: 99~99.9%

Tensile strength: equal to a forging

Elongation: slightly lower than a forging

【Typical SLM Material Properties】

316L stainless: σb=600MPa, δ=40%

Ti6Al4V: σb=1100MPa, δ=12%

AlSi10Mg: σb=400MPa, δ=8%

Inconel718: σb=1300MPa, δ=20%

【Design Guidelines】

1. Minimum wall thickness: 0.4~1mm (metal) / 0.8mm (plastic)

2. Minimum hole diameter: 0.5mm

3. Overhang angle: >45° (no support needed)

4. Tolerance: ±0.1~0.3mm

5. Surface Ra: 6~15μm (post processing needed)

6. Venting holes: a closed internal cavity needs a hole (to remove the powder)

7. Threads: printing them directly is rough, they need to be tapped

8. Mating surfaces: leave an allowance and then machine

【Post Processing】

1. Support removal (mechanical / chemical)

2. Shot blasting (improves the surface)

3. Heat treatment (stress relief ageing)

4. HIP hot isostatic pressing (eliminates the pores)

5. CNC finishing (the mating surfaces / the threads)

6. Polishing (lowers Ra)

7. Surface treatment (anodising / electroplating)

【Applications】

1. Aero engine blades / combustion chambers

2. Medical implants (hip joints / dental bridges)

3. Moulds (conformal cooling channels)

4. Complex lightweight structures (lattices)

5. Small batch customisation

6. Repair (DED)

【Advantages】

1. Complex shapes are formed in one setup

2. No tooling or moulds needed

3. A short cycle (hours to days)

4. A high degree of design freedom

5. High material utilisation (>90%)

6. Customised production

【Limitations】

1. Slow (hours to days)

2. Expensive (the metal powder is costly)

3. Size limited (a maximum of 500~1000mm)

4. A rough surface (post processing needed)

5. The mechanical properties are slightly lower than forgings

6. Cannot replace high volume production

Electrochemical Processing and Chemical Milling

【Chemical Milling】

The workpiece is immersed in a chemical solution

The metal is removed by chemical dissolution

Characteristics:

① No mechanical force (no stress deformation)

② Suited to thin walled parts

③ Complex shapes can be machined

④ Good surface quality

⑤ Slow

⑥ Deep structures cannot be machined

【Chemical Milling Process】

1. Clean the workpiece

2. Apply the protective coating (acid resistant rubber)

3. Pattern the mask (remove the protective coating where machining is required)

4. Chemical corrosion (NaOH / HCl / HF etc.)

5. Wash

6. Remove the protective coating

Corrosion rate: 0.02~0.05mm/min

Controlling the corrosion depth: by controlling the time

【Applications】

1. Thinning aluminium alloy skins (aerospace)

2. Etching printed circuit boards

3. Signs / name plates

4. Decorative patterns

5. Semiconductor manufacturing

【Electropolishing】

The workpiece acts as the anode and a current is passed in the electrolyte

The microscopic peaks on the surface dissolve preferentially

Characteristics:

① A bright surface (a mirror finish)

② No processing altered layer

③ It improves the corrosion resistance

④ It cannot change the shape

Parameters:

Current density: 10~100A/dm²

Temperature: 60~90℃

Time: 5~30min

Applications:

- Polishing stainless steel parts

- Medical equipment

- Food equipment

- Semiconductor parts

【Electrochemical Mechanical Machining】

Combines electrochemistry with mechanical grinding

Electrochemical dissolution + mechanical removal of the oxide film

Advantages:

① A higher efficiency than pure electrochemistry

② Good surface quality

③ Little tool wear

Applications:

- Turbine blades

- Stainless steel polishing

- Mould cavities

Wire EDM (WEDM) in Detail

【Classification of Wire EDM】

1. Fast wire (WEDM-HS)

Molybdenum wire (0.1~0.25mm)

A wire speed of 8~11m/s (a reciprocating cycle)

Emulsion / a dedicated fluid

Accuracy: ±0.01~0.02mm

Ra: 1.6~3.2μm

Commonly used in China

2. Slow wire (WEDM-LS)

Copper wire (0.1~0.3mm, single use)

A wire speed of 100~200m/min (one way)

Deionised water

Accuracy: ±0.003~0.008mm

Ra: 0.4~1.6μm (multiple cuts give Ra0.1)

Swiss / Japanese brands

3. Medium wire

Between the fast and the slow

Multiple cuts

Accuracy ±0.008~0.015

【Slow Wire Machining Parameters】

1. The first cut (rough)

Current: large

Speed: fast

Leave 0.05~0.1mm

2. The second cut (semi-finish)

Current: medium

Speed: medium

Leave 0.01~0.03mm

3. The third cut (finish)

Current: small

Speed: slow

Leave 0mm

4. The fourth cut (polishing)

Current: extremely small

Speed: extremely slow

Improves the surface quality

【Factors Influencing the Machining Accuracy】

1. Wire vibration (the wire tension control)

2. Wire wear (the slow wire is single use)

3. The dielectric fluid (the temperature / the conductivity)

4. Workpiece deformation (the residual stress)

5. The temperature (a temperature controlled workshop)

6. The machine accuracy

【Workpiece Materials】

Any conductive material

Commonly used:

Tool steel (Cr12MoV/D2)

Carbide

Stainless steel

Copper / aluminium

Titanium alloys

Diamond (with a conductive coating)

【Typical Applications】

1. Stamping mould punches and dies

2. Powder metallurgy dies

3. Wire drawing dies

4. Templates / gauges

5. Irregular holes / narrow grooves (0.1mm)

6. Gears / cams / templates

7. Aerospace precision parts

8. Micro machining (MEMS)

【Programs (G-Codes)】

Wire EDM mostly uses dedicated codes

G90: absolute coordinates

G91: incremental coordinates

G92: set the coordinates

T84: the fluid on

T85: the fluid off

T86: the wire on

T87: the wire off

M00: pause

The offset commands:

G41: left offset

G42: right offset

G40: cancel the offset

The offset value = the wire radius + the discharge gap

Example: a 0.18 wire + a 0.02 gap = 0.20

【Program Example】

Cutting a 10×10 square:

G90 G92 X0 Y0 (the start point)

T84 T86 (the fluid on, the wire on)

G42 D0.20 (right offset)

G01 X0 Y5

X10 Y5

X10 Y-5

X0 Y-5

X0 Y0

G40 (cancel the offset)

T85 T87 (the fluid off, the wire off)

M02 (end)

【Machining Techniques】

1. Preparing the start hole

- Drill a hole of 0.5~2mm

- Or pre-punch it (EDM hole punching)

2. Optimising the cutting path

- Avoid deformation (symmetrical cutting)

- Segment the cut (reduces the deformation)

- Leave a connecting tab and cut it last

3. Multiple cuts

- The slow wire must use multiple cuts

- It improves the accuracy and the surface

4. Workpiece clamping

- Support it fully (prevents deformation)

- Good electrical conduction

5. Wire tension control

- A constant tension (1~2N)

- Prevents fluttering

【Wire EDM vs Other Machining Processes】

Advantages:

① Any material hardness

② Complex contours

③ No cutting force

④ It can be machined after quenching

Disadvantages:

① Slow

② A surface altered layer

③ Only conductive materials

④ The corner radius is limited (the wire radius)

Related quick references: Machining FundamentalsCutting Tool MaterialsTool GeometryTurning ProcessMilling ProcessDrilling ProcessBoring ProcessGrinding ProcessMachining AllowanceProcess SequencingTypical ProcessesCNC ProgrammingFixture Design

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL