Knowledge Base › Design Pitfalls › Casting Pitfalls

Design Pitfalls · Casting Pitfalls (Quick-Reference Handbook)

Uneven Casting Wall Thickness

Pitfall: casting wall thickness varies too much, forming shrinkage cavities at the thick wall

Correct practice: keep the wall thickness as uniform as possible and blend different thicknesses with fillets

Reason: the thick wall cools slowly and solidifies last, forming shrinkage cavities

These principles must be followed in engineering design to avoid product failure or safety incidents caused by design oversight.

Casting Inner Wall Too Thick

Pitfall: the casting inner wall is thicker than the outer wall

Correct practice: make the inner-wall thickness 0.8× the outer wall

Reason: the inner wall dissipates heat slowly, prone to shrinkage porosity

These principles must be followed in engineering design to avoid product failure or safety incidents caused by design oversight.

Sharp Corners in Castings

Pitfall: the casting corners are designed as sharp corners

Correct practice: design all corners with a casting fillet R≥3mm

Reason: stress concentration at the sharp corner and poor mold filling

These principles must be followed in engineering design to avoid product failure or safety incidents caused by design oversight.

No Draft Angle

Pitfall: surfaces perpendicular to the parting plane have no draft angle

Correct practice: outer-wall draft 1°~3°, inner-wall draft 2°~5°

Reason: without draft the part cannot be ejected, or the surface is scored

These principles must be followed in engineering design to avoid product failure or safety incidents caused by design oversight.

Crossing Stiffening Ribs Forming a Hot Spot

Pitfall: stiffening ribs cross in a hash pattern, piling up metal at the intersection

Correct practice: stagger the ribs or provide a fillet transition

Reason: a hot spot forms at the intersection, prone to shrinkage porosity

These principles must be followed in engineering design to avoid product failure or safety incidents caused by design oversight.

Other quick references in this series:Welding PitfallsShaft System PitfallsSheet Metal PitfallsAssembly PitfallsHydraulic PitfallsPneumatic PitfallsShaft System DesignHousing DesignWelded StructuresSheet Metal StructuresSpring DesignBolted JointsBearing Arrangement

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL