1. Corrosion protection
2. Wear resistance
3. Decorative appearance
4. Special functions (conductive / insulating / reflective)
1. Blackening (bluing)
A Fe3O4 film forms on steel parts in an alkaline oxidising bath
Colour: black / blue black
Film thickness: 0.5~1.5μm
Corrosion protection: weak (oil must be applied)
Applications: general steel parts / fasteners / tools
Cost: low
2. Zinc plating
An electroplated zinc coating
Film thickness: 5~15μm
Corrosion protection: medium (white rust)
Passivation: coloured (hexavalent chrome) / blue white (trivalent chrome)
Applications: fasteners / stampings / automotive parts
Cost: medium
3. Nickel plating
An electroplated nickel coating
Film thickness: 5~25μm
Corrosion protection: medium (it is porous so a base layer is needed)
Decoration: silver white
Applications: decorative parts / wear parts / electroless nickel
Electroless Ni-P: uniform (it also works in deep holes)
4. Chrome plating
Decorative chrome: a Ni base layer + a Cr surface layer (0.3~0.5μm)
Hard chrome: Cr is plated directly (10~100μm)
Hardness: HV 800~1000
Wear resistance: excellent
Corrosion protection: medium (it is porous)
Applications: hydraulic cylinders / piston rods / moulds / gauges
Note: Cr⁶⁺ pollution (environmental restrictions)
5. Anodising (aluminium)
The aluminium is anodised in a sulphuric acid bath
Film thickness: 5~25μm (ordinary) / 25~100μm (hard)
Hard anodising HV 300~500
Colour: can be dyed (gold / red / blue / black)
Applications: aluminium parts for decoration / wear resistance / corrosion protection
Sealing: boiling water / nickel salt
6. Dacromet (Dacromet)
A zinc + aluminium flake + chromic acid coating
Film thickness: 5~15μm
Corrosion protection: excellent (>1000h salt spray)
No hydrogen embrittlement
Applications: automotive fasteners / outdoor parts
Cost: medium to high
7. Nitriding
Gas nitriding / ion nitriding
Film thickness: 0.2~0.6mm
Hardness: HV 900~1200
Wear resistance: excellent
Corrosion protection: good (it can replace stainless steel)
Applications: spindles / gears / moulds / cylinders
Material: 38CrMoAl / 40Cr
8. Carburising and quenching
Surface carburising + quenching
Film thickness: 0.5~1.5mm
Hardness: HRC 58~62
Wear resistance: excellent
Applications: gears / shafts / cams
Material: 20Cr / 20CrMnTi
9. Shot peening
Steel shot / glass beads strike the surface at high speed
Surface compressive stress (favourable for fatigue)
Hardened layer: 0.2~0.8mm
Applications: springs / gears / shafts / blades
10. Powder coating / painting
Electrostatic spraying + baking
Film thickness: 30~100μm
Colour: any
Applications: cabinets / steel structures / appliances
Corrosion protection: medium (it depends on the pretreatment)
11. Thermal spraying
Flame / arc / plasma spraying
Materials: zinc / aluminium / stainless steel / ceramic / tungsten carbide
Film thickness: 0.1~2mm
Applications: large steel structures / wear parts / repair
1. The corrosive environment
Dry indoors: blackening / oil
Outdoor atmosphere: zinc plating / Dacromet / painting
Marine: hot dip galvanising / multi layer coatings
Chemical: stainless steel / plastic lining / glass fibre reinforced plastic
2. The wear resistance requirement
General: hard chrome / nitriding
High: carburising / hard facing / thermal spraying of WC
3. Decoration
High gloss: chrome plating / polishing
Matte: sand blasting + anodising / painting
Coloured: anodising with dye / painting
4. Cost
Low: blackening
Medium: zinc plating / painting
High: chrome plating / Dacromet / nitriding
Very high: carburising / thermal spraying
Every surface treatment needs a pretreatment:
1. Degreasing (alkaline cleaning / solvent)
2. Derusting (acid pickling / sand blasting)
3. Activation (acid dipping)
4. Water rinsing
The pretreatment quality determines the adhesion strength
A heat source melts the coating material
It is sprayed at high speed onto the workpiece surface
A layered coating forms
Characteristics:
① A thick coating (0.1~5mm)
② A wide range of materials (metal / ceramic / plastic)
③ The workpiece does not melt (the temperature <200℃)
④ Worn parts can be repaired
⑤ Custom functional coatings can be produced
1. Flame spraying
An oxy-acetylene flame melts the wire / powder
Temperature: 3000℃
Speed: 50~100m/s
Coating bond: 5~30MPa (mechanical)
Suitable for: general purpose, large parts
2. Arc spraying
An arc between two wires melts them
Compressed air atomises the spray
Temperature: 4000~6000℃
Speed: 100~300m/s
Bond: 10~40MPa
Suitable for: large area corrosion protection of steel / aluminium / copper
High efficiency, low cost
3. Plasma spraying
A plasma arc melts the powder
Temperature: 10000~15000℃
Speed: 200~500m/s
Bond: 20~70MPa
Suitable for: ceramics / refractory metals
A dense coating of high quality
4. HVOF (High Velocity Oxy-Fuel Spraying)
High pressure combustion in a chamber
A Laval nozzle accelerates it to supersonic speed
Temperature: 2500~3000℃
Speed: 500~800m/s
Bond: 70~150MPa (the highest)
Suitable for: hard coatings such as WC/Co
A dense coating with residual compressive stress
5. D-Gun (explosion spraying)
An oxy-acetylene explosion
Speed: 800~1200m/s
Bond: the highest
Suitable for: high quality hard coatings
Expensive, there is little equipment
1. Metals
- Zinc / aluminium: corrosion protection (steel structures)
- Nickel / chromium: heat resistance
- Molybdenum: wear resistance
- Stainless steel: corrosion resistance
2. Alloys
- Nickel base (NiCrBSi): wear and corrosion resistance
- Cobalt base (Stellite): high temperature wear resistance
- Iron base: economical wear resistance
3. Ceramics
- Al2O3: insulation and wear resistance
- ZrO2: a thermal barrier coating
- Cr2O3: wear and corrosion resistance
4. Metal ceramics
- WC/Co: extremely wear resistant
- Cr3C2/NiCr: high temperature wear resistance
5. Composite powders
- Self lubricating (Ni/graphite)
- Ablative (aluminium/polyester)
1. Wear resistant coatings
- WC/Co (valves / guide rails)
- Al2O3 (guide plates / sealing rings)
- Cr2O3 (pump shafts / seals)
2. Corrosion resistant coatings
- Zinc / aluminium (steel structures / bridges)
- Stainless steel (chemical equipment)
- Hastelloy
3. Thermal barrier coatings
- ZrO2/Y2O3 (turbine blades)
- Provides 100~300℃ of insulation
4. Repair
- Worn journals (steel + nickel)
- Worn cylinder blocks (cast iron + nickel)
- Mould repair
5. Special functions
- Conductive (copper / silver)
- Insulating (Al2O3)
- Thermal insulation (ZrO2)
- Anti sticking (molybdenum)
1. Bond strength testing (tensile / shear)
2. Porosity (metallography)
3. Hardness (HV/HRC)
4. Thickness uniformity
5. Surface roughness
6. Wear testing
1. The pretreatment (sand blasting to Sa3)
2. The spraying parameters (temperature / speed / distance)
3. The powder quality (the particle size / the sphericity)
4. The workpiece temperature (<200℃)
5. Cooling (prevents overheating)
6. Post processing (sealing / remelting)